Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-4.301 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.063 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBaYF5 |
Band Gap6.495 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 261.1 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 195.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 195.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 261.1 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 309.4 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 154.7 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 261.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 154.7 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 163.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 156.3 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 261.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 312.6 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 232.1 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 209.4 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 232.1 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 261.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 65.3 |
BN (mp-984) | <1 0 1> | <1 0 1> | 121.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 309.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 309.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 195.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 154.7 |
Al (mp-134) | <1 1 1> | <1 0 0> | 261.1 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 156.3 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 326.4 |
SiC (mp-7631) | <1 1 0> | <1 0 1> | 242.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 326.4 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <0 0 1> | 156.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 156.3 |
C (mp-66) | <1 1 0> | <0 1 0> | 163.7 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 77.4 |
BN (mp-984) | <1 1 0> | <1 0 0> | 65.3 |
BN (mp-984) | <1 1 1> | <0 1 0> | 245.6 |
KP(HO2)2 (mp-23959) | <1 1 1> | <1 0 -1> | 154.7 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 326.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 226.4 |
PbS (mp-21276) | <1 1 0> | <1 0 -1> | 154.7 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 312.6 |
InP (mp-20351) | <1 1 0> | <1 0 -1> | 154.7 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 312.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 195.8 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 130.5 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 195.8 |
TeO2 (mp-2125) | <0 0 1> | <1 1 -1> | 225.3 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 -1> | 225.3 |
Ni (mp-23) | <1 0 0> | <1 1 0> | 209.4 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 154.7 |
Ni (mp-23) | <1 1 1> | <1 1 0> | 104.7 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 163.7 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 326.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaCuF5 (mvc-15792) | 0.1687 | 0.000 | 3 |
CaFeF5 (mvc-14316) | 0.2154 | 0.000 | 3 |
CaCrF5 (mvc-14169) | 0.0992 | 0.000 | 3 |
BaYCl5 (mp-755083) | 0.2189 | 0.042 | 3 |
CaCrF5 (mp-622572) | 0.0979 | 0.000 | 3 |
U2O5 (mp-647814) | 0.7091 | 0.017 | 2 |
Np2O5 (mp-554714) | 0.5744 | 0.000 | 2 |
U3O8 (mp-560402) | 0.6901 | 0.005 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Y_sv F |
Final Energy/Atom-6.5139 eV |
Corrected Energy-91.1941 eV
-91.1941 eV = -91.1941 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)