Final Magnetic Moment2.088 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.489 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa3Ti20O40 + Ba2Ti6O13 + Ba2Ti13O22 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/m [87] |
Hall-I 4 |
Point Group4/m |
Crystal Systemtetragonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 0> | 275.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 275.1 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 275.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 275.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 209.5 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 275.1 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 275.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 209.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 104.8 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 275.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 209.5 |
BN (mp-984) | <1 1 0> | <1 0 0> | 275.1 |
LiNbO3 (mp-3731) | <1 1 0> | <1 1 0> | 129.7 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 275.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 275.1 |
BN (mp-984) | <1 1 1> | <1 0 0> | 275.1 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 1> | 139.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 209.5 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 275.1 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 275.1 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 275.1 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 275.1 |
PbSe (mp-2201) | <1 1 1> | <1 0 0> | 275.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 209.5 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 259.3 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 275.1 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 183.4 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 259.3 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 275.1 |
CdSe (mp-2691) | <1 1 1> | <1 0 0> | 275.1 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 275.1 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 275.1 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 275.1 |
C (mp-48) | <0 0 1> | <1 0 0> | 275.1 |
YAlO3 (mp-3792) | <1 1 1> | <1 0 0> | 183.4 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 0> | 275.1 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <0 0 1> | 104.8 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 275.1 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 275.1 |
TiO2 (mp-390) | <1 0 1> | <1 0 0> | 275.1 |
GaSb (mp-1156) | <1 1 0> | <1 0 0> | 275.1 |
GaSb (mp-1156) | <1 1 1> | <1 0 0> | 275.1 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 104.8 |
Cu (mp-30) | <1 1 1> | <1 0 0> | 91.7 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 275.1 |
LiAlO2 (mp-3427) | <1 1 1> | <1 0 0> | 275.1 |
Fe2O3 (mp-24972) | <0 0 1> | <1 0 0> | 91.7 |
Fe2O3 (mp-24972) | <1 0 0> | <1 0 1> | 139.2 |
ZnTe (mp-2176) | <1 1 0> | <1 0 0> | 275.1 |
ZnTe (mp-2176) | <1 1 1> | <1 0 0> | 275.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn8PbO16 (mp-863883) | 0.3259 | 0.000 | 3 |
KMn6O12 (mp-761493) | 0.2191 | 0.000 | 3 |
KTi6O12 (mp-765472) | 0.2304 | 0.001 | 3 |
Ba(RuO2)6 (mp-561944) | 0.3388 | 0.020 | 3 |
CsTi6O12 (mp-867568) | 0.3465 | 0.000 | 3 |
Mn2Fe3Co3O16 (mp-772328) | 0.6088 | 0.109 | 4 |
V3Cr2Sb3O16 (mp-778794) | 0.6025 | 0.127 | 4 |
BaNb2(FeO3)4 (mp-1021950) | 0.2284 | 0.362 | 4 |
Ba2LiTi11O24 (mp-767384) | 0.4888 | 0.014 | 4 |
Ca2TiNb2O8 (mvc-71) | 0.5856 | 0.179 | 4 |
CoO2 (mvc-5816) | 0.5705 | 0.026 | 2 |
MnO2 (mvc-12283) | 0.5459 | 0.025 | 2 |
SnO2 (mvc-5659) | 0.5699 | 0.086 | 2 |
FeO2 (mvc-5967) | 0.5559 | 0.165 | 2 |
VO2 (mvc-12071) | 0.5546 | 0.082 | 2 |
LaZnCrWO6 (mvc-9890) | 0.6720 | 0.167 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Ti_pv O |
Final Energy/Atom-8.7582 eV |
Corrected Energy-349.6651 eV
-349.6651 eV = -332.8101 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|