Final Magnetic Moment7.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.771 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.046 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGdAsO4 |
Band Gap1.187 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 -1> | 207.6 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 156.6 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 210.0 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 324.4 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 139.0 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 350.2 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 70.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 174.6 |
BaF2 (mp-1029) | <1 0 0> | <1 1 -1> | 207.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 70.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 174.6 |
GaAs (mp-2534) | <1 0 0> | <1 1 -1> | 259.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 139.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 231.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 163.4 |
KCl (mp-23193) | <1 0 0> | <1 1 -1> | 207.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 279.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 -1> | 259.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 -1> | 139.0 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 139.0 |
GaN (mp-804) | <1 0 1> | <1 1 -1> | 155.7 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 303.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 261.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 185.4 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 303.5 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 336.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 208.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 252.0 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 231.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 303.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 171.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 163.4 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 244.4 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 104.7 |
ZnSe (mp-1190) | <1 0 0> | <1 1 -1> | 259.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 139.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 139.6 |
Te2W (mp-22693) | <1 1 0> | <1 1 1> | 114.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 52.2 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 46.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 69.8 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 156.6 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 349.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 209.5 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 168.0 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 261.1 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 324.4 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 252.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 324.4 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 168.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaGaH4 (mp-23918) | 0.3515 | 0.000 | 3 |
Dy2(SeO4)3 (mp-769213) | 0.3689 | 0.079 | 3 |
CaSO4 (mp-4406) | 0.3501 | 0.000 | 3 |
BaWO4 (mp-1095315) | 0.3532 | 0.021 | 3 |
BiPO4 (mp-558798) | 0.2992 | 0.006 | 3 |
CaU(PO4)2 (mp-9360) | 0.2892 | 0.000 | 4 |
Er2SiSO4 (mp-555990) | 0.4233 | 0.020 | 4 |
SrTlVO4 (mp-566556) | 0.4095 | 0.000 | 4 |
KY(PSe3)2 (mp-571057) | 0.4069 | 0.000 | 4 |
NaNdSiO4 (mp-13774) | 0.4257 | 0.000 | 4 |
TlCl2 (mp-27205) | 0.5845 | 0.000 | 2 |
TlBr2 (mp-27398) | 0.5347 | 0.000 | 2 |
InI2 (mp-29312) | 0.4833 | 0.000 | 2 |
InBr2 (mp-568108) | 0.5077 | 0.000 | 2 |
GaCl2 (mp-568848) | 0.4831 | 0.000 | 2 |
KCaNd(PO4)2 (mp-676934) | 0.4194 | 0.000 | 5 |
K2HoPWO8 (mp-565678) | 0.3567 | 0.000 | 5 |
K2YbMoPO8 (mp-565817) | 0.3498 | 0.003 | 5 |
K2BiMoPO8 (mp-566924) | 0.3509 | 0.000 | 5 |
K2BiPWO8 (mp-566769) | 0.3549 | 0.001 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Gd As O |
Final Energy/Atom-8.7244 eV |
Corrected Energy-110.3112 eV
-110.3112 eV = -104.6928 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)