Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.678 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.073 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.26 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Si2O5 + CuO + SiO2 |
Band Gap0.444 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 276.9 |
AlN (mp-661) | <1 0 1> | <1 -1 0> | 163.2 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 301.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 226.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 215.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 301.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 221.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 332.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 332.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 177.8 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 276.9 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 276.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 332.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 215.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 274.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 226.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 274.3 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 276.9 |
BN (mp-984) | <0 0 1> | <1 -1 -1> | 250.7 |
BN (mp-984) | <1 0 0> | <0 1 -1> | 174.7 |
BN (mp-984) | <1 0 1> | <0 1 1> | 177.8 |
BN (mp-984) | <1 1 0> | <1 0 0> | 301.4 |
BN (mp-984) | <1 1 1> | <1 -1 -1> | 167.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 301.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 306.4 |
LiF (mp-1138) | <1 1 0> | <1 -1 -1> | 167.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 221.5 |
Al (mp-134) | <1 1 0> | <1 0 0> | 301.4 |
Al (mp-134) | <1 1 1> | <1 0 -1> | 306.4 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 301.4 |
Ag (mp-124) | <1 1 0> | <1 -1 -1> | 167.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 332.3 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 221.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 221.5 |
SiC (mp-7631) | <0 0 1> | <1 0 -1> | 306.4 |
MgO (mp-1265) | <1 0 0> | <1 -1 0> | 163.2 |
MgO (mp-1265) | <1 1 0> | <1 -1 -1> | 250.7 |
TiO2 (mp-2657) | <1 0 0> | <0 1 -1> | 262.1 |
TiO2 (mp-2657) | <1 0 1> | <1 -1 -1> | 250.7 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 332.3 |
C (mp-66) | <1 0 0> | <0 1 0> | 205.7 |
C (mp-66) | <1 1 0> | <1 0 0> | 301.4 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 1> | 215.6 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 226.0 |
GdScO3 (mp-5690) | <1 0 1> | <0 1 0> | 274.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 221.5 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 205.7 |
C (mp-48) | <1 0 0> | <0 1 -1> | 174.7 |
C (mp-48) | <1 1 0> | <1 0 -1> | 229.8 |
WSe2 (mp-1821) | <0 0 1> | <1 -1 -1> | 250.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr4(PO4)3 (mp-504357) | 0.6683 | 0.784 | 3 |
Cu4(PO4)3 (mp-26742) | 0.6287 | 0.028 | 3 |
V2(CuO2)5 (mp-559440) | 0.6529 | 0.033 | 3 |
Mn2Si4O11 (mp-768088) | 0.6470 | 0.090 | 3 |
Cr4(PO4)3 (mp-773959) | 0.6685 | 0.784 | 3 |
LiMnSi3O8 (mp-761967) | 0.4833 | 0.085 | 4 |
Li2Cr2Si5O13 (mp-761646) | 0.3160 | 0.015 | 4 |
Li2Fe2Si5O13 (mp-761475) | 0.4520 | 0.188 | 4 |
LiSi3BiO8 (mp-757127) | 0.4571 | 0.095 | 4 |
LiCu2P3O10 (mp-26531) | 0.4810 | 0.049 | 4 |
Na3LiMg4(Si2O5)6 (mp-695366) | 0.5735 | 0.710 | 5 |
LiFeP2HO7 (mp-850985) | 0.6481 | 0.061 | 5 |
Rb9Na2Al11Si13O48 (mp-720212) | 0.6971 | 0.114 | 5 |
Cs2Li2B2P4O15 (mp-1019606) | 0.7282 | 0.000 | 5 |
Na6Al4Fe(Si4O13)2 (mp-705484) | 0.7252 | 0.033 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv Si O |
Final Energy/Atom-6.9660 eV |
Corrected Energy-324.7650 eV
-324.7650 eV = -306.5055 eV (uncorrected energy) - 18.2595 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)