Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.546 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.039 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.33 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCd2Si(P2O7)2 |
Band Gap3.937 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 206.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 209.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 289.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 137.3 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 260.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 206.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 206.0 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 206.0 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 209.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 68.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 289.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 274.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 130.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 104.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 137.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 137.3 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 206.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 289.0 |
BN (mp-984) | <1 0 1> | <1 0 0> | 206.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 96.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 137.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 68.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 96.3 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 206.0 |
TiO2 (mp-2657) | <1 1 1> | <1 0 1> | 260.7 |
LaF3 (mp-905) | <1 1 1> | <1 0 0> | 206.0 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 274.6 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 1> | 130.4 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 -1> | 104.8 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 -1> | 209.7 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 0> | 206.0 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 274.6 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 274.6 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 274.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 192.6 |
C (mp-66) | <1 1 0> | <1 0 0> | 274.6 |
Si (mp-149) | <1 1 0> | <1 0 0> | 206.0 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 1> | 130.4 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 -1> | 104.8 |
Mg (mp-153) | <0 0 1> | <1 0 -1> | 104.8 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 206.0 |
Mg (mp-153) | <1 1 1> | <1 0 -1> | 209.7 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 137.3 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 0> | 137.3 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 0> | 137.3 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 206.0 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 206.0 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 137.3 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 206.0 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 96.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr(PO3)2 (mp-775457) | 0.5341 | 0.022 | 3 |
Cr(PO4)2 (mp-697815) | 0.4893 | 0.141 | 3 |
Hg(PO3)2 (mp-15994) | 0.4119 | 0.000 | 3 |
Cd(PO3)2 (mp-4659) | 0.4722 | 0.000 | 3 |
Mn2P3O10 (mp-31981) | 0.5389 | 0.029 | 3 |
Li2Cr(PO3)4 (mp-774367) | 0.4288 | 0.077 | 4 |
LiFe(PO3)3 (mp-699324) | 0.4172 | 0.032 | 4 |
LiSb2P5O16 (mp-684104) | 0.4251 | 0.047 | 4 |
LiCu(PO3)4 (mp-26262) | 0.3942 | 0.000 | 4 |
LiMn(PO3)4 (mp-695788) | 0.4253 | 0.015 | 4 |
NaLiCu(PO3)3 (mp-775900) | 0.6039 | 0.086 | 5 |
RbLiV(PO4)2 (mp-764302) | 0.5621 | 0.058 | 5 |
KEu2Si4O10F (mp-561529) | 0.6627 | 0.000 | 5 |
MnFeCo(PO4)3 (mp-763446) | 0.7173 | 0.026 | 5 |
NaZnFe2(PO4)3 (mp-566178) | 0.6668 | 0.005 | 5 |
CsAlBP2HO9 (mp-542129) | 0.6432 | 0.000 | 6 |
RbAlBP2HO9 (mp-542130) | 0.6859 | 0.000 | 6 |
CsFeBP2HO9 (mp-761395) | 0.6770 | 0.000 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cd Si P O |
Final Energy/Atom-6.7395 eV |
Corrected Energy-302.7212 eV
-302.7212 eV = -283.0570 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)