Final Magnetic Moment0.333 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.479 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.064 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSn3(PO4)2 + LiSn2(PO4)3 + Li3PO4 |
Band Gap0.252 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 143.4 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 170.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 239.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 -1> | 185.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 115.7 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 239.1 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 231.4 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 231.4 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 1> | 143.4 |
MgO (mp-1265) | <1 0 0> | <0 1 1> | 143.4 |
C (mp-66) | <1 1 1> | <1 0 0> | 247.2 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 115.7 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 1> | 191.4 |
PbS (mp-21276) | <1 0 0> | <0 1 1> | 143.4 |
InP (mp-20351) | <1 0 0> | <0 1 1> | 143.4 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 1> | 143.4 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 1> | 191.4 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 239.1 |
SiC (mp-11714) | <1 0 1> | <0 1 0> | 231.4 |
C (mp-48) | <1 0 0> | <1 1 1> | 191.4 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 318.8 |
WS2 (mp-224) | <1 0 0> | <0 1 0> | 231.4 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 239.1 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 115.7 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 239.1 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 -1> | 185.5 |
Cu (mp-30) | <1 1 1> | <1 0 0> | 247.2 |
LiAlO2 (mp-3427) | <1 1 0> | <1 1 -1> | 185.5 |
LiAlO2 (mp-3427) | <1 0 0> | <0 1 0> | 231.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn7(PO4)6 (mp-770696) | 0.6701 | 0.008 | 3 |
Cr5(PO4)4 (mp-540446) | 0.6258 | 0.007 | 3 |
Cr5(PO4)4 (mp-775246) | 0.6220 | 0.007 | 3 |
V7(PO4)6 (mp-769607) | 0.6792 | 0.017 | 3 |
Cr7(PO4)6 (mp-505154) | 0.6790 | 0.002 | 3 |
Li2V5(PO4)4 (mp-763552) | 0.5640 | 0.076 | 4 |
Li3Sn3(PO4)4 (mp-758156) | 0.4341 | 0.076 | 4 |
LiFe5P3O13 (mp-762666) | 0.5538 | 0.051 | 4 |
Li3Sb3(PO4)4 (mp-758651) | 0.4274 | 0.067 | 4 |
Li2Ni5(PO4)4 (mp-540465) | 0.5556 | 0.043 | 4 |
LiVPHO5 (mp-767213) | 0.5198 | 0.000 | 5 |
LiCrPHO5 (mp-765883) | 0.5206 | 0.000 | 5 |
LiFePHO5 (mp-771864) | 0.5319 | 0.000 | 5 |
Li4V2P4H3O16 (mp-765418) | 0.5504 | 0.025 | 5 |
LiCoPHO5 (mp-770053) | 0.5500 | 0.030 | 5 |
Li2VCrP2(HO5)2 (mp-765060) | 0.4928 | 0.001 | 6 |
Li2VFeP2(HO5)2 (mp-765061) | 0.4960 | 0.002 | 6 |
Li2VCrP2(HO5)2 (mp-763880) | 0.4968 | 0.001 | 6 |
Li2MnVP2(HO5)2 (mp-777149) | 0.4910 | 0.022 | 6 |
Li2VCrP2(HO5)2 (mp-765059) | 0.4970 | 0.001 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Sn_d P O |
Final Energy/Atom-6.5947 eV |
Corrected Energy-548.0949 eV
-548.0949 eV = -514.3849 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)