Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.503 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.072 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiPO3 + LiSn2(PO3)5 |
Band Gap4.334 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 163.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 275.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 229.2 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 156.7 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 153.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 229.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 320.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 320.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 320.8 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 137.5 |
BN (mp-984) | <0 0 1> | <1 0 1> | 163.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 229.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 229.2 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 229.2 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 275.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 320.8 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 320.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 320.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 320.8 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 320.8 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 320.8 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 229.2 |
MoSe2 (mp-1634) | <1 0 1> | <0 0 1> | 320.8 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 275.0 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 91.7 |
Au (mp-81) | <1 0 0> | <0 0 1> | 320.8 |
Au (mp-81) | <1 1 0> | <0 0 1> | 320.8 |
C (mp-48) | <1 0 0> | <0 0 1> | 229.2 |
C (mp-48) | <1 0 1> | <0 0 1> | 183.3 |
C (mp-48) | <1 1 0> | <0 0 1> | 229.2 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 229.2 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 229.2 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 137.5 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 320.8 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 229.2 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 275.0 |
ZrO2 (mp-2858) | <1 1 1> | <1 -1 0> | 156.1 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 229.2 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 229.2 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 183.3 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 320.8 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 320.8 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 183.3 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 320.8 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 320.8 |
CdWO4 (mp-19387) | <1 1 1> | <1 0 -1> | 156.7 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 229.2 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 229.2 |
TiO2 (mp-390) | <1 0 1> | <1 0 -1> | 156.7 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 229.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Y(PO3)3 (mp-686038) | 0.5116 | 0.481 | 3 |
Sn(PO3)3 (mp-684482) | 0.6151 | 0.125 | 3 |
Sr2P6O17 (mp-27583) | 0.5652 | 0.000 | 3 |
NaPO3 (mp-4734) | 0.6360 | 0.008 | 3 |
Sn(PO3)3 (mp-26172) | 0.5417 | 0.088 | 3 |
LiSb(PO3)4 (mp-759485) | 0.5000 | 0.065 | 4 |
LiFe(PO3)4 (mp-763626) | 0.5442 | 0.214 | 4 |
LiBiP2O7 (mp-760629) | 0.5616 | 0.065 | 4 |
LiSn2(PO3)5 (mp-26949) | 0.5282 | 0.000 | 4 |
LiFe(PO3)4 (mp-762548) | 0.5139 | 0.208 | 4 |
Rb2EuGa(SiO3)4 (mp-684467) | 0.7330 | 0.129 | 5 |
CsUGa(PO5)2 (mp-559852) | 0.7288 | 0.000 | 5 |
K2CeAl(SiO3)4 (mp-1019774) | 0.7005 | 0.000 | 5 |
CaP3H10NO12 (mp-705854) | 0.7454 | 0.054 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Sn_d P O |
Final Energy/Atom-6.7697 eV |
Corrected Energy-476.2960 eV
-476.2960 eV = -446.7998 eV (uncorrected energy) - 29.4962 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)