Final Magnetic Moment1.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.187 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.041 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2CuP2O7 + CuO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPna21 [33] |
HallP 2c 2n |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 1> | 61.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 138.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 231.9 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 204.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 172.9 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 185.4 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 308.8 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 231.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 311.3 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 86.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 138.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 247.0 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 204.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 311.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 276.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 255.8 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 308.8 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 258.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 69.1 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 258.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 231.9 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 138.2 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 276.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 247.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 204.6 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 153.5 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 172.9 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 231.9 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 204.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 103.8 |
Te2W (mp-22693) | <1 0 0> | <0 1 1> | 308.8 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 255.8 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 242.1 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 231.9 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 231.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 172.9 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 231.9 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 204.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 207.4 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 247.0 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 204.6 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 308.8 |
Te2Mo (mp-602) | <1 1 0> | <0 1 1> | 185.3 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 308.8 |
BN (mp-984) | <0 0 1> | <0 1 0> | 153.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 242.1 |
BN (mp-984) | <1 0 0> | <0 1 0> | 153.5 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 1 0> | 258.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 153.5 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 204.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn2SiO4 (mp-3789) | 0.4032 | 0.000 | 3 |
Be(GaO2)2 (mp-676950) | 0.3974 | 0.116 | 3 |
Zn2SiO4 (mp-1020594) | 0.3241 | 0.010 | 3 |
Li2SO4 (mp-4556) | 0.2900 | 0.000 | 3 |
Li2BeF4 (mp-4622) | 0.3801 | 0.000 | 3 |
LiMnPO4 (mp-861484) | 0.1481 | 0.014 | 4 |
LiFePO4 (mp-540123) | 0.1467 | 0.012 | 4 |
LiCoPO4 (mp-761727) | 0.0929 | 0.006 | 4 |
LiFePO4 (mp-761474) | 0.0903 | 0.433 | 4 |
LiFePO4 (mp-761484) | 0.1543 | 0.012 | 4 |
BN (mp-1077506) | 0.7153 | 0.302 | 2 |
Cr3N4 (mp-1014369) | 0.7122 | 0.164 | 2 |
SiC2 (mp-1019097) | 0.5840 | 0.562 | 2 |
CN2 (mp-1077595) | 0.6623 | 0.691 | 2 |
Ti3N4 (mp-1080190) | 0.6919 | 0.118 | 2 |
Li4Ga3Si3IO12 (mp-557112) | 0.5290 | 0.000 | 5 |
Li4Ga3Si3ClO12 (mp-554203) | 0.5849 | 0.000 | 5 |
Li4Ga3Si3BrO12 (mp-556649) | 0.5633 | 0.000 | 5 |
Mn4Be3Ge3SeO12 (mp-25766) | 0.6313 | 0.000 | 5 |
Mn4Be3Ge3SO12 (mp-25772) | 0.6285 | 0.000 | 5 |
Na2Li2Al3Si3ClO12 (mp-43030) | 0.6094 | 0.003 | 6 |
C (mp-568410) | 0.5920 | 0.507 | 1 |
C (mp-1008374) | 0.6919 | 0.437 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv P O |
Final Energy/Atom-6.2446 eV |
Corrected Energy-185.8418 eV
Uncorrected energy = -174.8498 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Corrected energy = -185.8418 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)