Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.627 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.070 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAgF + LiF |
Band Gap2.645 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 194.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 229.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 291.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 229.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 152.9 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 291.3 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 229.3 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 291.3 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 291.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 76.4 |
BN (mp-984) | <1 1 0> | <1 0 1> | 134.4 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 229.3 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 291.8 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 291.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 152.9 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 305.7 |
C (mp-48) | <1 1 0> | <0 1 1> | 135.4 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 229.3 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 152.9 |
CaCO3 (mp-3953) | <1 1 1> | <0 0 1> | 152.9 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 229.3 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 0> | 194.2 |
SiC (mp-8062) | <1 1 0> | <0 1 0> | 291.3 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 229.3 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 291.8 |
CdWO4 (mp-19387) | <1 1 1> | <1 1 -1> | 155.3 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 229.3 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 291.3 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 229.3 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 194.2 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 152.9 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 152.9 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 291.8 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 229.3 |
Ga2O3 (mp-886) | <1 0 -1> | <1 1 1> | 189.1 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 291.3 |
Au (mp-81) | <1 0 0> | <0 1 0> | 291.3 |
Cu (mp-30) | <1 1 1> | <0 1 0> | 291.3 |
LiAlO2 (mp-3427) | <1 0 0> | <1 -1 0> | 233.9 |
Fe2O3 (mp-24972) | <0 0 1> | <0 1 0> | 291.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2Hg5Se8 (mp-685952) | 0.6906 | 0.025 | 3 |
Li10Ti4O13 (mp-772260) | 0.6352 | 0.070 | 3 |
Li2AgF4 (mp-760781) | 0.6870 | 0.038 | 3 |
Li6Ag3F10 (mp-760133) | 0.5860 | 0.063 | 3 |
Li6Cu5F14 (mp-760015) | 0.6974 | 0.061 | 3 |
LiCrPO4 (mp-773992) | 0.7181 | 0.060 | 4 |
Li2CrSiO4 (mp-762303) | 0.7183 | 0.094 | 4 |
LiNiPO4 (mp-762152) | 0.7280 | 0.099 | 4 |
Li4Mn3OF8 (mp-764336) | 0.7088 | 0.077 | 4 |
LiNiPO4 (mp-763130) | 0.6351 | 0.063 | 4 |
Cu11S16 (mp-675278) | 0.6556 | 0.237 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ag F |
Final Energy/Atom-4.4072 eV |
Corrected Energy-282.0616 eV
-282.0616 eV = -282.0616 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)