Final Magnetic Moment0.213 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.908 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 129.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 280.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 259.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 280.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 237.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 237.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 216.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 280.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 194.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 172.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 172.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 280.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 172.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 194.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 108.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 237.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 172.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 43.2 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 120.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 324.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 216.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 324.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 367.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 86.4 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 263.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 302.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 108.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 43.2 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 120.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 302.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 86.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 345.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 64.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 194.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 345.5 |
BN (mp-984) | <1 1 1> | <0 0 1> | 280.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 172.8 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 129.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 280.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 108.0 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 280.8 |
MoS2 (mp-1434) | <1 0 1> | <0 0 1> | 280.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 86.4 |
Al (mp-134) | <1 1 0> | <0 0 1> | 324.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 302.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 1> | 244.4 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 280.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 240.5 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 43.2 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 120.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ErZrSb (mp-5848) | 0.1945 | 0.000 | 3 |
DyZrSb (mp-5068) | 0.2009 | 0.000 | 3 |
YZrSb (mp-31438) | 0.2081 | 0.000 | 3 |
TbZrSb (mp-4075) | 0.2129 | 0.000 | 3 |
HoZrSb (mp-3346) | 0.1928 | 0.000 | 3 |
Pr2Sb (mp-1071848) | 0.0678 | 0.000 | 2 |
La2Sb (mp-759) | 0.0488 | 0.000 | 2 |
La2Bi (mp-1077063) | 0.0794 | 0.000 | 2 |
Nd2Bi (mp-1071453) | 0.0715 | 0.000 | 2 |
Pr2Bi (mp-1077777) | 0.0751 | 0.018 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Sb |
Final Energy/Atom-5.5754 eV |
Corrected Energy-33.4523 eV
-33.4523 eV = -33.4523 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)