@article{Donohue1970, author = "Donohue, P.C. and Young, H.S.", title = "Synthesis, structure, and superconductivity of new high pressure phases in the systems ge - p and ge - as", journal = "Journal of Solid State Chemistry", year = "1970", volume = "1", pages = "143-149", ASTM_id = "JSSCBI" }