Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.462 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.062 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.38 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSbPO4 + Li3PO4 |
Band Gap3.612 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 252.6 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 119.4 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 252.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 168.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 84.2 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 119.4 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 252.6 |
SiC (mp-11714) | <1 0 1> | <1 0 1> | 197.2 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 139.6 |
C (mp-48) | <1 0 0> | <0 1 0> | 116.3 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 -1> | 119.4 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 -1> | 238.7 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 1> | 197.2 |
ZnO (mp-2133) | <0 0 1> | <0 1 0> | 232.7 |
Cu (mp-30) | <1 1 0> | <1 0 0> | 168.4 |
Fe2O3 (mp-24972) | <1 1 0> | <1 0 0> | 252.6 |
Fe2O3 (mp-24972) | <1 1 1> | <1 0 0> | 252.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 84.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 84.2 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 119.4 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 252.6 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 252.6 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 139.6 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 252.6 |
LiTaO3 (mp-3666) | <1 1 1> | <1 0 0> | 252.6 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 232.7 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 252.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr4P2O9 (mp-773396) | 0.5967 | 0.230 | 3 |
Na17Al5O16 (mp-559916) | 0.6242 | 0.002 | 3 |
Ca3(AlN2)2 (mp-570505) | 0.6363 | 0.002 | 3 |
Ca5Ge3O11 (mp-774105) | 0.5710 | 0.016 | 3 |
Mn4(PO4)3 (mp-32010) | 0.6354 | 0.142 | 3 |
Li4Cu7(PO4)6 (mp-761936) | 0.5521 | 0.086 | 4 |
Li3Bi2(PO4)3 (mp-684042) | 0.3163 | 0.044 | 4 |
NaSbMoO5 (mp-637336) | 0.4658 | 0.032 | 4 |
LiMn4(PO4)3 (mp-32021) | 0.4793 | 0.046 | 4 |
CaV2(PO4)2 (mvc-9882) | 0.3971 | 0.093 | 4 |
Li4Mn5Sn(PO4)6 (mp-853140) | 0.5690 | 0.078 | 5 |
LiMn3P2(HO3)4 (mp-763726) | 0.5952 | 0.479 | 5 |
Na2LiVPO6 (mp-763825) | 0.5336 | 0.094 | 5 |
SrMgMn(PO4)2 (mvc-2987) | 0.5833 | 0.018 | 5 |
SrMgFe(PO4)2 (mvc-3019) | 0.5704 | 0.015 | 5 |
Li4Mn3NbV2(PO4)6 (mp-770640) | 0.5713 | 0.095 | 6 |
Li4Cr2Ni3Sn(PO4)6 (mp-778614) | 0.6085 | 0.183 | 6 |
Li4Mn3NbCr2(PO4)6 (mp-776566) | 0.5336 | 0.102 | 6 |
Li4TiMn3Cr2(PO4)6 (mp-778261) | 0.6332 | 0.081 | 6 |
Li4Mn2Fe3Sb(PO4)6 (mp-776752) | 0.6086 | 3.420 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Sb P O |
Final Energy/Atom-6.5208 eV |
Corrected Energy-277.6889 eV
-277.6889 eV = -260.8339 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)