Final Magnetic Moment16.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.489 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LiF (mp-1138) | <1 0 0> | <0 0 1> | 268.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 268.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 268.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 268.8 |
GaN (mp-804) | <1 1 0> | <1 -1 1> | 175.9 |
LiNbO3 (mp-3731) | <1 1 0> | <0 1 0> | 127.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 268.8 |
MoS2 (mp-1434) | <0 0 1> | <1 -1 1> | 175.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 173.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 268.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 -1 1> | 175.9 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 268.8 |
LiTaO3 (mp-3666) | <1 1 0> | <0 1 0> | 127.5 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 179.2 |
GdScO3 (mp-5690) | <0 1 0> | <1 -1 1> | 175.9 |
Mg (mp-153) | <0 0 1> | <1 -1 1> | 175.9 |
Mg (mp-153) | <1 0 0> | <1 -1 -1> | 183.1 |
Mg (mp-153) | <1 1 0> | <1 -1 1> | 175.9 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 268.8 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 268.8 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 -1> | 173.1 |
TiO2 (mp-2657) | <1 1 1> | <0 1 -1> | 145.6 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 -1> | 173.1 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 255.1 |
WS2 (mp-224) | <0 0 1> | <1 -1 1> | 175.9 |
C (mp-48) | <1 0 1> | <0 0 1> | 179.2 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 179.2 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 268.8 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 268.8 |
TiO2 (mp-390) | <0 0 1> | <1 0 -1> | 173.1 |
TiO2 (mp-390) | <1 1 1> | <0 0 1> | 268.8 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 268.8 |
SrTiO3 (mp-4651) | <1 0 0> | <1 -1 1> | 175.9 |
CaF2 (mp-2741) | <1 1 0> | <1 -1 1> | 175.9 |
Fe2O3 (mp-24972) | <1 1 0> | <0 1 0> | 127.5 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 268.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La6Mn5O18 (mp-698577) | 0.3253 | 0.009 | 3 |
La10Mn9O30 (mp-698607) | 0.3418 | 0.009 | 3 |
La10Mn9O30 (mp-761747) | 0.3381 | 0.010 | 3 |
Ba13Bi11O36 (mp-758120) | 0.3106 | 0.000 | 3 |
Ba8(Bi2O7)3 (mp-867542) | 0.2888 | 0.000 | 3 |
La10Mg(Ga3O10)3 (mp-695030) | 0.4672 | 0.047 | 4 |
Ba2SrWO6 (mp-19078) | 0.4747 | 0.001 | 4 |
Ba2PrNbO6 (mp-552176) | 0.4928 | 0.001 | 4 |
Ba2SrUO6 (mp-1079113) | 0.4469 | 0.009 | 4 |
Ba2LaTaO6 (mp-13056) | 0.4889 | 0.000 | 4 |
CaLa9Ti5Cr5O30 (mp-694926) | 0.5299 | 0.061 | 5 |
Ca2La8Ti5Cr5O30 (mp-743953) | 0.5385 | 0.044 | 5 |
SrLaMnRuO6 (mp-39239) | 0.4402 | 0.000 | 5 |
SrLaMnRuO6 (mp-690590) | 0.4669 | 0.000 | 5 |
SrLaCuRuO6 (mp-677659) | 0.4740 | 0.024 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv U O |
Final Energy/Atom-8.2723 eV |
Corrected Energy-608.5552 eV
-608.5552 eV = -579.0590 eV (uncorrected energy) - 29.4962 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)