Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.180 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNb2O5 + TiO2 |
Band Gap2.047 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 0 1> | 318.9 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 222.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 318.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 318.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 239.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 318.9 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 239.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 259.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 173.5 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 260.3 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 258.9 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 129.4 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 264.2 |
GaSe (mp-1943) | <1 0 0> | <0 1 -1> | 138.0 |
GaSe (mp-1943) | <1 0 1> | <0 1 1> | 280.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 239.2 |
Mg (mp-153) | <0 0 1> | <0 1 1> | 280.0 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 318.9 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 239.2 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 280.0 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 159.4 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 260.3 |
TeO2 (mp-2125) | <0 1 0> | <0 1 1> | 280.0 |
TeO2 (mp-2125) | <1 0 0> | <0 1 1> | 280.0 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 0> | 173.5 |
Ni (mp-23) | <1 1 0> | <1 1 1> | 258.9 |
PbSe (mp-2201) | <1 1 1> | <0 1 0> | 260.3 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 318.9 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 239.2 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 239.2 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 264.2 |
C (mp-66) | <1 1 0> | <1 0 -1> | 143.7 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 1> | 186.7 |
GdScO3 (mp-5690) | <1 0 1> | <0 1 0> | 173.5 |
Au (mp-81) | <1 0 0> | <0 1 1> | 280.0 |
CdSe (mp-2691) | <1 1 1> | <0 1 0> | 260.3 |
WS2 (mp-224) | <0 0 1> | <0 1 1> | 280.0 |
ZrO2 (mp-2858) | <1 1 0> | <1 -1 -1> | 159.6 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 1> | 280.0 |
YAlO3 (mp-3792) | <1 1 0> | <0 1 1> | 280.0 |
ZrO2 (mp-2858) | <1 1 -1> | <0 0 1> | 318.9 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 159.4 |
MgF2 (mp-1249) | <1 0 1> | <0 1 1> | 186.7 |
ZnO (mp-2133) | <1 0 1> | <0 1 1> | 280.0 |
ZnO (mp-2133) | <1 1 1> | <0 1 0> | 260.3 |
GaSb (mp-1156) | <1 1 1> | <0 1 0> | 260.3 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 318.9 |
Cu (mp-30) | <1 1 0> | <0 1 0> | 260.3 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 239.2 |
ZnO (mp-2133) | <0 0 1> | <0 1 0> | 260.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2WO5 (mp-761287) | 0.6001 | 0.059 | 3 |
TiNb2O7 (mp-758243) | 0.2511 | 0.022 | 3 |
V3CoO8 (mp-776864) | 0.5861 | 0.248 | 3 |
Nb18P3O50 (mp-772038) | 0.5956 | 0.063 | 3 |
TiV3O8 (mp-849354) | 0.5731 | 0.029 | 3 |
Li2V4O5F8 (mp-764711) | 0.5643 | 0.073 | 4 |
BaNb3NO7 (mp-776461) | 0.7011 | 0.063 | 4 |
Nb2O5 (mp-680944) | 0.3107 | 0.000 | 2 |
V3O7 (mp-773443) | 0.3530 | 0.024 | 2 |
Nb2O5 (mp-556048) | 0.4191 | 0.007 | 2 |
Nb12O29 (mp-510554) | 0.2602 | 0.000 | 2 |
Nb12O29 (mp-1470) | 0.3009 | 0.000 | 2 |
Hg12SbBr(ClO3)2 (mp-642625) | 0.7163 | 0.032 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv Nb_pv O |
Final Energy/Atom-8.9620 eV |
Corrected Energy-567.2154 eV
-567.2154 eV = -537.7193 eV (uncorrected energy) - 29.4962 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)