Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.537 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiSn2(PO4)3 |
Band Gap3.430 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 1 1> | 246.8 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 232.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 63.1 |
GaN (mp-804) | <1 1 1> | <0 1 -1> | 274.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 246.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 136.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 106.1 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 232.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 -1 1> | 156.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 189.3 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 106.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 63.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 -1 0> | 276.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 252.4 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 123.4 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 232.0 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 212.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 252.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 315.6 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 189.3 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 232.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 315.6 |
MoS2 (mp-1434) | <0 0 1> | <0 1 -1> | 274.4 |
Al (mp-134) | <1 0 0> | <1 -1 0> | 276.1 |
Al (mp-134) | <1 1 0> | <0 1 0> | 232.0 |
Al (mp-134) | <1 1 1> | <0 0 1> | 252.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 246.8 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 252.4 |
TeO2 (mp-2125) | <0 1 0> | <1 0 1> | 212.3 |
SiC (mp-7631) | <0 0 1> | <1 0 -1> | 233.3 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 189.3 |
Mg (mp-153) | <0 0 1> | <0 1 -1> | 274.4 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 189.3 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 315.6 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 154.7 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 63.1 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 273.5 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 63.1 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 273.5 |
BaTiO3 (mp-5986) | <0 0 1> | <1 -1 0> | 276.1 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 68.4 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 1> | 212.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 189.3 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 252.4 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 273.5 |
SiC (mp-11714) | <0 0 1> | <1 0 -1> | 233.3 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 0> | 257.3 |
MoSe2 (mp-1634) | <1 0 1> | <1 0 0> | 273.5 |
Ag (mp-124) | <1 1 0> | <0 1 -1> | 274.4 |
BN (mp-984) | <0 0 1> | <1 -1 1> | 312.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr3(P2O7)2 (mp-569271) | 0.3847 | 0.001 | 3 |
MnV2O6 (mp-777555) | 0.3970 | 0.000 | 3 |
V2FeO6 (mp-773218) | 0.4046 | 0.020 | 3 |
Cr3(P2O7)2 (mp-774562) | 0.3873 | 0.001 | 3 |
MnV5O12 (mp-776190) | 0.3822 | 0.061 | 3 |
LiFe(SO4)2 (mp-850472) | 0.1965 | 0.025 | 4 |
LiCr(SO4)2 (mp-861585) | 0.1781 | 0.023 | 4 |
LiSn2(PO4)3 (mp-27094) | 0.1787 | 0.001 | 4 |
LiSn2(PO4)3 (mp-27122) | 0.1766 | 0.003 | 4 |
LiNi2(PO4)3 (mp-697786) | 0.1933 | 0.162 | 4 |
CrO2 (mvc-11581) | 0.6635 | 0.166 | 2 |
VO2 (mp-777469) | 0.6468 | 0.038 | 2 |
Cr5O12 (mp-19575) | 0.6347 | 0.025 | 2 |
VO2 (mvc-6918) | 0.5987 | 0.094 | 2 |
MoO2 (mvc-6944) | 0.5672 | 0.281 | 2 |
LiMgCr3(SO4)6 (mp-769554) | 0.2755 | 0.227 | 5 |
Li3Cr13Ni3(SO4)24 (mp-743984) | 0.2830 | 0.009 | 5 |
LiCr3Ni(SO4)6 (mp-767547) | 0.2948 | 0.008 | 5 |
Li2MnV(PO4)3 (mp-770169) | 0.3196 | 0.022 | 5 |
LiMgCr3(SO4)6 (mp-694995) | 0.2088 | 0.226 | 5 |
NaLi5Ti3Cr3(PO4)9 (mp-744549) | 0.5009 | 0.059 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.3630 | 0.255 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.3185 | 0.011 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.4498 | 0.020 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.4450 | 0.330 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6280 | 0.002 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Sn_d P O |
Final Energy/Atom-6.8211 eV |
Corrected Energy-262.4135 eV
-262.4135 eV = -245.5585 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)