Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.468 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.006 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi7O5F11 + BiF3 |
Band Gap3.290 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 237.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 203.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 33.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 237.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 135.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 33.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 237.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 203.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 305.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 305.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 338.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 67.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 169.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 237.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 338.9 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 207.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 305.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 305.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 33.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 169.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 237.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 218.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 135.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 109.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 305.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 271.1 |
GaSe (mp-1943) | <1 0 1> | <0 1 0> | 207.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 271.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 169.5 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 203.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 33.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 169.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 338.9 |
Al (mp-134) | <1 1 0> | <0 0 1> | 67.8 |
Al (mp-134) | <1 1 1> | <0 0 1> | 169.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 271.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 305.0 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 237.2 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 237.2 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 207.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 338.9 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 203.3 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 214.1 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 101.7 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 305.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 237.2 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 224.6 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 271.1 |
C (mp-66) | <1 1 0> | <0 0 1> | 203.3 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 1> | 218.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Bi2OF4 (mp-753309) | 0.4584 | 0.012 | 3 |
BaLaBr5 (mp-770392) | 0.5821 | 0.074 | 3 |
BaLaCl5 (mp-770125) | 0.5978 | 0.076 | 3 |
Bi3NF6 (mp-28946) | 0.5550 | 0.029 | 3 |
Nd3S2Br5 (mp-28297) | 0.5091 | 0.020 | 3 |
BaYbCdSb2 (mp-865143) | 0.7482 | 0.000 | 4 |
Nb2Tl3CuSe12 (mp-570757) | 0.7219 | 0.000 | 4 |
KSr2Cd2Sb3 (mp-866639) | 0.6581 | 0.000 | 4 |
P3Pd7 (mp-505363) | 0.5977 | 0.000 | 2 |
Mg6Si5 (mp-1073904) | 0.5974 | 0.183 | 2 |
Mg4Si3 (mp-1074264) | 0.5904 | 0.152 | 2 |
Mg4Si3 (mp-1074404) | 0.5619 | 0.133 | 2 |
Mg4Si3 (mp-1074562) | 0.5488 | 0.187 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Bi O F |
Final Energy/Atom-5.1929 eV |
Corrected Energy-222.4506 eV
Uncorrected energy = -207.7146 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-0.462 eV/atom x 20.0 atoms) = -9.2400 eV
Corrected energy = -222.4506 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)