Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.472 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.054 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSbPO4 + LiPO3 |
Band Gap3.393 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 251.8 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 251.8 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 251.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 306.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 269.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 306.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 79.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 167.8 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 239.0 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 245.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 239.0 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 159.4 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 79.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 318.7 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 202.4 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 83.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 306.7 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 239.0 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 269.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 269.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 202.4 |
GaSe (mp-1943) | <1 0 1> | <1 1 0> | 207.9 |
BN (mp-984) | <1 0 1> | <0 1 1> | 182.4 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 -1> | 239.0 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 1> | 273.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 -1> | 159.4 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 0> | 306.7 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 1> | 129.8 |
LiTaO3 (mp-3666) | <1 1 1> | <1 0 0> | 251.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 269.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 83.9 |
TiO2 (mp-2657) | <1 1 1> | <1 0 -1> | 239.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 269.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 83.9 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 207.9 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 269.9 |
Ni (mp-23) | <1 0 0> | <0 1 1> | 273.6 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 259.6 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 159.4 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 251.8 |
PbSe (mp-2201) | <1 0 0> | <1 0 -1> | 79.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 202.4 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 306.7 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 129.8 |
Al (mp-134) | <1 0 0> | <0 1 1> | 182.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 306.7 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 -1> | 201.1 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 269.9 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 135.0 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 251.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cd2P2O7 (mp-27686) | 0.5799 | 0.000 | 3 |
Li2Cr2O7 (mp-770862) | 0.6001 | 0.034 | 3 |
Cr2P2O7 (mp-705599) | 0.5165 | 0.000 | 3 |
Cu2P3O10 (mp-26532) | 0.5799 | 0.041 | 3 |
V2P2O7 (mp-776066) | 0.6033 | 0.130 | 3 |
LiMnP2O7 (mp-782650) | 0.4434 | 0.236 | 4 |
LiMnP2O7 (mp-762788) | 0.4843 | 0.178 | 4 |
Li2Sn(PO3)4 (mp-26271) | 0.5221 | 0.021 | 4 |
MgCrP2O7 (mvc-6967) | 0.5344 | 0.444 | 4 |
ZnCrP2O7 (mvc-6971) | 0.4486 | 0.015 | 4 |
Li2V2SiGeO10 (mp-771932) | 0.7104 | 0.046 | 5 |
LiAg2P3(HO5)2 (mp-695951) | 0.6360 | 0.020 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Sb P O |
Final Energy/Atom-6.7072 eV |
Corrected Energy-314.7824 eV
-314.7824 eV = -295.1183 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)