Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-2.482 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.081 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBiPO4 + LiBi(PO3)4 |
Band Gap3.959 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 0> | 267.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 267.1 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 279.9 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 251.4 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 284.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 -1> | 282.6 |
AlN (mp-661) | <0 0 1> | <0 1 -1> | 282.6 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 265.6 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 284.9 |
AlN (mp-661) | <1 1 1> | <0 1 -1> | 141.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 267.9 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 279.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 279.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 267.1 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 284.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 89.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 284.9 |
CdS (mp-672) | <1 0 0> | <0 1 -1> | 141.3 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 251.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 189.9 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 267.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 267.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 267.9 |
BN (mp-984) | <1 1 1> | <1 0 0> | 267.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 178.1 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 -1> | 284.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 267.9 |
Ag (mp-124) | <1 1 1> | <1 -1 1> | 214.4 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 284.9 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 1> | 125.7 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 284.9 |
BN (mp-984) | <1 0 0> | <0 1 -1> | 211.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 267.9 |
TeO2 (mp-2125) | <1 1 0> | <0 1 -1> | 282.6 |
TiO2 (mp-2657) | <0 0 1> | <0 1 -1> | 282.6 |
TiO2 (mp-2657) | <1 0 1> | <0 1 -1> | 282.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 133.9 |
TiO2 (mp-2657) | <1 1 1> | <1 1 1> | 172.9 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 267.1 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 -1> | 284.9 |
MgO (mp-1265) | <1 1 1> | <1 -1 1> | 214.4 |
GdScO3 (mp-5690) | <1 0 1> | <0 1 0> | 279.9 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 267.1 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 267.1 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 0> | 279.9 |
Mg (mp-153) | <1 1 0> | <1 0 -1> | 284.9 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 267.9 |
Ni (mp-23) | <1 0 0> | <0 1 -1> | 282.6 |
Ni (mp-23) | <1 1 1> | <0 1 0> | 209.9 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 -1> | 284.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2Ni3P9O28 (mp-868306) | 0.3349 | 0.088 | 4 |
Li2Fe3P9O28 (mp-762680) | 0.3489 | 0.052 | 4 |
Li2V3P9O28 (mp-763445) | 0.2971 | 0.056 | 4 |
Li2Mn3P9O28 (mp-763668) | 0.3568 | 0.053 | 4 |
Li2Cr3P9O28 (mp-779220) | 0.3142 | 0.061 | 4 |
VO2 (mvc-6918) | 0.6983 | 0.100 | 2 |
FeO2 (mvc-11999) | 0.6683 | 0.354 | 2 |
Cr19O48 (mp-850874) | 0.5544 | 0.095 | 2 |
Cr5O12 (mp-19575) | 0.6547 | 0.025 | 2 |
VO2 (mp-776137) | 0.6895 | 0.099 | 2 |
In2P2O7 (mp-17100) | 0.3986 | 0.000 | 3 |
Ni4P7O24 (mp-504245) | 0.4370 | 0.091 | 3 |
Ni(PO3)3 (mp-699315) | 0.4088 | 0.071 | 3 |
Sn(PO3)2 (mp-767192) | 0.4350 | 0.022 | 3 |
V5(P3O11)2 (mp-767351) | 0.4286 | 0.020 | 3 |
LiCr3Ni(SO4)6 (mp-767547) | 0.4888 | 0.009 | 5 |
Li3Cr13Ni3(SO4)24 (mp-743984) | 0.4717 | 0.010 | 5 |
LiMgCr3(SO4)6 (mp-694995) | 0.4816 | 0.008 | 5 |
VCrP2(HO5)2 (mp-766804) | 0.4795 | 0.050 | 5 |
VFeP2(HO5)2 (mp-765969) | 0.4644 | 0.053 | 5 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5564 | 0.040 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.4896 | 0.001 | 6 |
KFeBP2HO9 (mp-635134) | 0.6016 | 0.142 | 6 |
RbScBP2HO9 (mp-23809) | 0.5470 | 0.000 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5931 | 0.020 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6562 | 0.002 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points32 |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Bi P O |
Final Energy/Atom-6.8304 eV |
Corrected Energy-306.5414 eV
-306.5414 eV = -286.8772 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction)
|