material

Li4CuF7

ID:

mp-759877

DOI:

10.17188/1291522


Material Details

Final Magnetic Moment
2.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.664 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.040 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.56 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Li3CuF6 + LiF
Band Gap
0.686 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
F43m [216]
Hall
F 4 2 3
Point Group
43m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ni (mp-23) <1 1 0> <1 1 0> 0.000 295.6
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.000 278.7
Cu (mp-30) <1 1 0> <1 1 0> 0.000 295.6
Au (mp-81) <1 0 0> <1 0 0> 0.000 69.7
Au (mp-81) <1 1 0> <1 1 0> 0.000 98.5
Au (mp-81) <1 1 1> <1 1 1> 0.000 120.7
Al (mp-134) <1 0 0> <1 0 0> 0.005 278.7
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.006 278.7
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.007 120.7
GaN (mp-804) <1 0 1> <1 0 0> 0.008 209.0
Ag (mp-124) <1 0 0> <1 0 0> 0.008 69.7
Ag (mp-124) <1 1 0> <1 1 0> 0.009 98.5
Ag (mp-124) <1 1 1> <1 1 1> 0.009 120.7
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.012 295.6
C (mp-66) <1 1 0> <1 1 0> 0.017 197.1
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.018 278.7
SiC (mp-8062) <1 1 0> <1 1 0> 0.020 295.6
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.026 139.4
NdGaO3 (mp-3196) <0 0 1> <1 0 0> 0.029 278.7
Mg (mp-153) <1 0 1> <1 0 0> 0.032 209.0
ZrO2 (mp-2858) <1 1 0> <1 0 0> 0.043 278.7
GaN (mp-804) <1 1 1> <1 0 0> 0.047 278.7
LiF (mp-1138) <1 0 0> <1 0 0> 0.061 278.7
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.064 278.7
InP (mp-20351) <1 0 0> <1 0 0> 0.071 69.7
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.072 139.4
InP (mp-20351) <1 1 0> <1 1 0> 0.077 98.5
GaP (mp-2490) <1 0 0> <1 0 0> 0.092 278.7
C (mp-48) <0 0 1> <1 1 0> 0.101 295.6
BaTiO3 (mp-5986) <0 0 1> <1 1 1> 0.108 241.4
Mg (mp-153) <1 1 1> <1 0 0> 0.113 278.7
ZnO (mp-2133) <1 1 1> <1 0 0> 0.122 278.7
Ni (mp-23) <1 1 1> <1 0 0> 0.127 209.0
KTaO3 (mp-3614) <1 0 0> <1 1 1> 0.133 241.4
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.161 278.7
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.164 278.7
LiNbO3 (mp-3731) <1 0 0> <1 1 0> 0.174 295.6
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.200 209.0
GaTe (mp-542812) <0 0 1> <1 1 0> 0.214 295.6
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.216 139.4
Si (mp-149) <1 0 0> <1 0 0> 0.245 278.7
PbS (mp-21276) <1 0 0> <1 0 0> 0.248 69.7
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.252 278.7
PbS (mp-21276) <1 1 0> <1 1 0> 0.268 98.5
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.366 69.7
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.396 98.5
MgAl2O4 (mp-3536) <1 1 1> <1 1 1> 0.406 120.7
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.425 69.7
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.459 98.5
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.462 295.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
62 49 49 0 0 0
49 62 49 0 0 0
49 49 62 0 0 0
0 0 0 25 0 0
0 0 0 0 25 0
0 0 0 0 0 25
Compliance Tensor Sij (10-12Pa-1)
51.4 -22.6 -22.6 0 0 0
-22.6 51.4 -22.6 0 0 0
-22.6 -22.6 51.4 0 0 0
0 0 0 40.4 0 0
0 0 0 0 40.4 0
0 0 0 0 0 40.4
Shear Modulus GV
18 GPa
Bulk Modulus KV
53 GPa
Shear Modulus GR
12 GPa
Bulk Modulus KR
53 GPa
Shear Modulus GVRH
15 GPa
Bulk Modulus KVRH
53 GPa
Elastic Anisotropy
2.33
Poisson's Ratio
0.37

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 -0.37718 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 -0.37718 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 -0.37718
Piezoelectric Modulus ‖eijmax
0.37718 C/m2
Crystallographic Direction vmax
0.00000
1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
2.43 0.00 0.00
0.00 2.43 0.00
0.00 0.00 2.43
Dielectric Tensor εij (total)
4.59 0.00 0.00
0.00 4.59 0.00
0.00 0.00 4.59
Polycrystalline dielectric constant εpoly
(electronic contribution)
2.43
Polycrystalline dielectric constant εpoly
(total)
4.59
Refractive Index n
1.56
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Be4TeO7 (mp-27608) 0.3939 0.000 3
Li4MnF7 (mp-763783) 0.0487 0.041 3
Li4VF7 (mp-762800) 0.0520 0.013 3
LiFeF3 (mp-777393) 0.6073 0.044 3
Ga4GeO8 (mp-29455) 0.6339 0.000 3
LiFeOF2 (mp-850136) 0.7069 0.040 4
LiVCuO4 (mp-764692) 0.7257 0.071 4
LiMnOF2 (mp-777099) 0.6156 0.023 4
LiVOF2 (mp-765452) 0.6533 0.021 4
MgCr(GeO3)2 (mvc-8398) 0.7294 0.674 4
Fe5O8 (mp-543082) 0.6923 0.163 2
Al2O3 (mp-7048) 0.6264 0.009 2
Ga2O3 (mp-886) 0.6394 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Cu_pv F
Final Energy/Atom
-4.4877 eV
Corrected Energy
-57.0858 eV
Uncorrected energy = -53.8518 eV Composition-based energy adjustment (-0.462 eV/atom x 7.0 atoms) = -3.2340 eV Corrected energy = -57.0858 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)