Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.652 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.22 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.060 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 289.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 310.4 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 235.4 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 193.2 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 253.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 258.6 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 289.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 111.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 206.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 258.6 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 96.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 310.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 310.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 206.9 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 310.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 258.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 258.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 258.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 1> | 253.9 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 296.1 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 289.8 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 155.2 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 289.8 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 1> | 215.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 206.9 |
TiO2 (mp-2657) | <1 1 0> | <1 1 1> | 253.9 |
C (mp-66) | <1 0 0> | <0 1 0> | 193.2 |
C (mp-66) | <1 1 0> | <1 0 0> | 197.4 |
GdScO3 (mp-5690) | <1 1 1> | <0 0 1> | 206.9 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 310.4 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 258.6 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 258.6 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 310.4 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 206.9 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 258.6 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 296.1 |
CaCO3 (mp-3953) | <1 0 0> | <1 1 1> | 253.9 |
LaF3 (mp-905) | <1 0 1> | <0 1 1> | 215.7 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 258.6 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 0> | 193.2 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 310.4 |
TbScO3 (mp-31119) | <1 1 1> | <0 0 1> | 206.9 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 310.4 |
TiO2 (mp-390) | <0 0 1> | <0 1 0> | 289.8 |
TiO2 (mp-390) | <1 0 0> | <1 1 1> | 253.9 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 258.6 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 258.6 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 310.4 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 310.4 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 289.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Si(H3C)2 (mp-978595) | 0.6799 | 0.056 | 3 |
H22C10O3 (mp-707910) | 0.5312 | 0.075 | 3 |
PH4N3 (mp-28892) | 0.6263 | 0.000 | 3 |
AlSCl7 (mp-555805) | 0.6687 | 0.000 | 3 |
BH6N (mp-675418) | 0.7250 | 0.012 | 3 |
H10S(NO)4 (mp-707020) | 0.5908 | 0.123 | 4 |
AlH3NCl3 (mp-759356) | 0.6641 | 0.000 | 4 |
H8S2N2O5 (mp-706653) | 0.5915 | 0.075 | 4 |
P2H12N7Cl (mp-758356) | 0.6583 | 0.010 | 4 |
Li3P11(H3N)17 (mp-722502) | 0.6103 | 0.005 | 4 |
H34C19 (mp-866659) | 0.7263 | 0.060 | 2 |
PH10SN3O2 (mp-707041) | 0.6394 | 0.026 | 5 |
AlPH8(CCl2)2 (mp-569751) | 0.6121 | 0.000 | 5 |
MnH21C7S3N (mp-557785) | 0.4897 | 0.118 | 5 |
K2HS2NO6 (mp-695383) | 0.5395 | 0.024 | 5 |
AgH11C4(SO)3 (mp-560182) | 0.6136 | 0.153 | 5 |
KLiH4S2(NO3)2 (mp-699460) | 0.6079 | 0.053 | 6 |
Si3PH27C9BrN2 (mp-567146) | 0.6721 | 0.115 | 6 |
P2H19C6I2NCl4 (mp-567256) | 0.6542 | 0.034 | 6 |
TeH12AuC4S3N (mp-560718) | 0.5269 | 0.098 | 6 |
SiP3H29C10BrN (mp-24830) | 0.6272 | 0.063 | 6 |
SiPH18C6INCl (mp-738707) | 0.5739 | 0.083 | 7 |
LiBeH8CNOF4 (mp-560581) | 0.7037 | 0.038 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv P H S N |
Final Energy/Atom-4.9385 eV |
Corrected Energy-329.9236 eV
-329.9236 eV = -325.9428 eV (uncorrected energy) - 3.9808 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)