Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.797 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBaSO4 + BaS |
Band Gap4.975 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 299.5 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 164.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 190.4 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 164.2 |
LiNbO3 (mp-3731) | <1 1 0> | <0 1 0> | 130.3 |
Al (mp-134) | <1 0 0> | <0 1 1> | 164.2 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 190.4 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 190.4 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 299.5 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 260.6 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 1> | 190.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 299.5 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 164.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 299.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 99.8 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 260.6 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 199.6 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 299.5 |
C (mp-66) | <1 1 0> | <0 1 1> | 164.2 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 299.5 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 1> | 190.4 |
PbSe (mp-2201) | <1 1 0> | <0 1 1> | 164.2 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 299.5 |
Si (mp-149) | <1 0 0> | <0 0 1> | 299.5 |
CdSe (mp-2691) | <1 1 0> | <0 1 1> | 164.2 |
WS2 (mp-224) | <1 1 0> | <1 0 0> | 162.0 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 199.6 |
SiC (mp-8062) | <1 1 0> | <0 1 1> | 164.2 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 299.5 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 299.5 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 299.5 |
ZnO (mp-2133) | <1 1 0> | <0 0 1> | 299.5 |
ZnO (mp-2133) | <1 1 1> | <1 0 1> | 190.4 |
GaSb (mp-1156) | <1 1 0> | <0 1 1> | 164.2 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 299.5 |
ZnTe (mp-2176) | <1 1 0> | <0 1 1> | 164.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv S O |
Final Energy/Atom-6.4978 eV |
Corrected Energy-643.3510 eV
-643.3510 eV = -591.3006 eV (uncorrected energy) - 52.0505 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)