material

Li3VS4

ID:

mp-760375

DOI:

10.17188/1291614


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.441 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
1.57 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.895 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P43m [215]
Hall
P 4 2 3
Point Group
43m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Mg (mp-153) <0 0 1> <1 1 1> 0.000 61.4
InP (mp-20351) <1 1 1> <1 1 1> 0.000 61.4
InP (mp-20351) <1 1 0> <1 1 0> 0.000 50.2
InP (mp-20351) <1 0 0> <1 0 0> 0.000 35.5
LiF (mp-1138) <1 0 0> <1 0 0> 0.000 283.7
CdS (mp-672) <0 0 1> <1 1 1> 0.001 61.4
Ni (mp-23) <1 0 0> <1 0 0> 0.001 319.2
Ge(Bi3O5)4 (mp-23352) <1 1 1> <1 1 1> 0.001 184.3
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.001 150.5
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.002 61.4
WS2 (mp-224) <0 0 1> <1 1 1> 0.003 61.4
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.005 319.2
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.005 319.2
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.005 177.3
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.006 248.3
InSb (mp-20012) <1 0 0> <1 0 0> 0.008 177.3
SiC (mp-8062) <1 1 0> <1 1 0> 0.009 300.9
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.010 61.4
C (mp-66) <1 1 0> <1 1 0> 0.011 200.6
CdTe (mp-406) <1 0 0> <1 0 0> 0.011 177.3
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.015 319.2
AlN (mp-661) <1 0 1> <1 1 0> 0.015 250.8
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.016 184.3
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.016 184.3
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.016 319.2
AlN (mp-661) <1 1 1> <1 1 0> 0.017 200.6
YVO4 (mp-19133) <1 0 0> <1 1 1> 0.017 184.3
LaF3 (mp-905) <0 0 1> <1 1 1> 0.019 184.3
AlN (mp-661) <1 1 0> <1 1 0> 0.020 300.9
ZnO (mp-2133) <1 1 1> <1 0 0> 0.022 283.7
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.023 212.8
BaTiO3 (mp-5986) <1 0 0> <1 1 1> 0.025 307.2
Bi2Se3 (mp-541837) <1 0 0> <1 0 0> 0.029 248.3
PbS (mp-21276) <1 1 1> <1 1 1> 0.030 61.4
GaN (mp-804) <1 0 1> <1 0 0> 0.031 212.8
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.031 177.3
MgO (mp-1265) <1 1 1> <1 0 0> 0.031 248.3
PbS (mp-21276) <1 1 0> <1 1 0> 0.032 50.2
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.033 283.7
Cu (mp-30) <1 1 0> <1 1 0> 0.034 150.5
Ni (mp-23) <1 1 0> <1 1 0> 0.035 300.9
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.037 150.5
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.037 141.9
PbS (mp-21276) <1 0 0> <1 0 0> 0.038 35.5
GaN (mp-804) <0 0 1> <1 1 0> 0.039 250.8
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.040 283.7
Au (mp-81) <1 1 0> <1 1 0> 0.044 50.2
Ni (mp-23) <1 1 1> <1 0 0> 0.047 106.4
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.048 200.6
AlN (mp-661) <0 0 1> <1 0 0> 0.050 177.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
32 3 3 0 0 0
3 32 3 0 0 0
3 3 32 0 0 0
0 0 0 4 0 0
0 0 0 0 4 0
0 0 0 0 0 4
Compliance Tensor Sij (10-12Pa-1)
32.2 -3.2 -3.2 0 0 0
-3.2 32.2 -3.2 0 0 0
-3.2 -3.2 32.2 0 0 0
0 0 0 264.3 0 0
0 0 0 0 264.3 0
0 0 0 0 0 264.3
Shear Modulus GV
8 GPa
Bulk Modulus KV
13 GPa
Shear Modulus GR
5 GPa
Bulk Modulus KR
13 GPa
Shear Modulus GVRH
7 GPa
Bulk Modulus KVRH
13 GPa
Elastic Anisotropy
2.40
Poisson's Ratio
0.28

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.07079 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 0.07079 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 0.07079
Piezoelectric Modulus ‖eijmax
0.07079 C/m2
Crystallographic Direction vmax
0.00000
1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
3.17 0.00 0.00
0.00 3.17 0.00
0.00 0.00 3.17
Dielectric Tensor εij (total)
4.14 0.00 0.00
0.00 4.14 0.00
0.00 0.00 4.14
Polycrystalline dielectric constant εpoly
(electronic contribution)
3.17
Polycrystalline dielectric constant εpoly
(total)
4.14
Refractive Index n
1.78
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li3NbS4 (mp-755309) 0.1946 0.010 3
Ag3PS4 (mp-12459) 0.6400 0.000 3
Li3CrS4 (mp-753982) 0.0570 0.050 3
NaFeS2 (mp-28100) 0.6083 0.177 3
Li3SbS4 (mp-850275) 0.3201 0.071 3
Li2CoBO4 (mp-778655) 0.5652 0.078 4
Li2FeBO4 (mp-769698) 0.4937 0.109 4
Li2FeBO4 (mp-769696) 0.5686 0.045 4
Li2NiBO4 (mp-769685) 0.5629 0.090 4
Li2CoBO4 (mp-778539) 0.5361 0.287 4
SnN (mvc-13927) 0.6383 0.298 2
Si (mp-16220) 0.6400 0.338 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv V_pv S
Final Energy/Atom
-5.0288 eV
Corrected Energy
-42.8839 eV
-42.8839 eV = -40.2301 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)