Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.399 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.017 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRhO2 + Ta2O5 + Rh |
Band Gap1.017 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41md [109] |
HallI 4bw 2 |
Point Group4mm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 229.3 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 123.3 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 184.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 123.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 206.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 206.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 229.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 206.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 329.7 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 288.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 308.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 275.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 183.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 246.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 229.3 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 222.5 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 246.6 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 246.6 |
Te2W (mp-22693) | <1 0 0> | <1 1 1> | 296.6 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 174.8 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 288.5 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 174.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 206.0 |
GaSe (mp-1943) | <1 1 0> | <1 0 1> | 123.3 |
BN (mp-984) | <0 0 1> | <1 1 0> | 174.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 229.3 |
BN (mp-984) | <1 0 1> | <1 1 1> | 222.5 |
BN (mp-984) | <1 1 0> | <1 0 0> | 247.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 184.9 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 206.0 |
Al (mp-134) | <1 0 0> | <1 0 1> | 246.6 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 233.1 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 45.9 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 61.6 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 229.3 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 1> | 184.9 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 1> | 123.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 91.7 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 206.0 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 123.6 |
TiO2 (mp-2657) | <0 0 1> | <1 1 0> | 174.8 |
TiO2 (mp-2657) | <1 0 0> | <1 1 1> | 222.5 |
TiO2 (mp-2657) | <1 0 1> | <1 0 1> | 308.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 137.6 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 123.6 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 229.3 |
C (mp-66) | <1 0 0> | <0 0 1> | 229.3 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 275.1 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 288.5 |
Mg (mp-153) | <1 0 0> | <1 1 1> | 148.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
-0.65070 | -0.30695 | -0.30695 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.53982 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.53982 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.78221 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
9.48 | 0.00 | 0.00 |
0.00 | 9.23 | 0.00 |
0.00 | 0.00 | 9.23 |
Dielectric Tensor εij (total) |
||
---|---|---|
21.81 | 0.00 | -0.00 |
0.00 | 30.20 | 0.00 |
-0.00 | 0.00 | 30.20 |
Polycrystalline dielectric constant
εpoly∞
9.31
|
Polycrystalline dielectric constant
εpoly
27.40
|
Refractive Index n3.05 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TiNbO4 (mp-756350) | 0.1386 | 0.042 | 3 |
TaTiO4 (mp-760439) | 0.1459 | 0.008 | 3 |
TaAlO4 (mp-760396) | 0.1309 | 0.056 | 3 |
NbRhO4 (mp-756638) | 0.0908 | 0.015 | 3 |
TaVO4 (mp-772246) | 0.1214 | 0.000 | 3 |
Ta2CrNO5 (mp-782717) | 0.2163 | 0.068 | 4 |
LiFe3(OF3)2 (mp-779990) | 0.1942 | 0.005 | 4 |
LiV3(OF3)2 (mp-868491) | 0.2169 | 0.000 | 4 |
Ta2CrNO5 (mp-849938) | 0.2124 | 0.071 | 4 |
Ta2CrNO5 (mp-849504) | 0.1823 | 0.065 | 4 |
MoO2 (mp-715509) | 0.1425 | 0.000 | 2 |
VO2 (mp-714875) | 0.1530 | 0.000 | 2 |
MoO2 (mp-715476) | 0.1386 | 0.000 | 2 |
MoO2 (mp-715550) | 0.1487 | 0.037 | 2 |
WO2 (mp-715508) | 0.1447 | 0.030 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ta_pv Rh_pv O |
Final Energy/Atom-8.4331 eV |
Corrected Energy-106.8158 eV
-106.8158 eV = -101.1975 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)