Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.879 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.022 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.80 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTb2O3 + ZrO2 |
Band Gap2.713 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <1 0 0> | 112.7 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 195.2 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 195.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 195.2 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 159.4 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 159.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 225.4 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 159.4 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 225.4 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 195.2 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 159.4 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 112.7 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 159.4 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 1 1> | 195.2 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 225.4 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 225.4 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 112.7 |
Au (mp-81) | <1 0 0> | <1 0 0> | 225.4 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 225.4 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 225.4 |
C (mp-48) | <0 0 1> | <1 1 1> | 195.2 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 112.7 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 1> | 195.2 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 159.4 |
CdSe (mp-2691) | <1 1 1> | <1 1 1> | 195.2 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 112.7 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 112.7 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 1 0> | 159.4 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 112.7 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 112.7 |
YAlO3 (mp-3792) | <1 0 0> | <1 1 0> | 159.4 |
TiO2 (mp-390) | <1 0 1> | <1 1 0> | 159.4 |
GaTe (mp-542812) | <1 0 0> | <1 0 0> | 225.4 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 159.4 |
GaSb (mp-1156) | <1 1 1> | <1 1 1> | 195.2 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 159.4 |
ZnTe (mp-2176) | <1 1 1> | <1 1 1> | 195.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Er2Sn2O7 (mp-3688) | 0.0085 | 0.000 | 3 |
Ho2Sn2O7 (mp-3884) | 0.0164 | 0.000 | 3 |
Er2Tc2O7 (mp-557806) | 0.0174 | 0.118 | 3 |
Tb2Pt2O7 (mp-754768) | 0.0038 | 0.000 | 3 |
Y2Zr2O7 (mp-558411) | 0.0084 | 0.060 | 3 |
Mn2Hg2SF6 (mp-600275) | 0.5221 | 0.465 | 4 |
Zn2Hg2OF6 (mp-17972) | 0.5142 | 0.000 | 4 |
Mn2Hg2SF6 (mp-556900) | 0.5068 | 0.465 | 4 |
Ni2Hg2OF6 (mp-540834) | 0.5900 | 0.000 | 4 |
Ca2Ta2O6F (mp-14560) | 0.2022 | 0.076 | 4 |
GdTi2CdO6F (mp-695048) | 0.4974 | 0.142 | 5 |
YTi2CdO6F (mp-686765) | 0.5338 | 0.142 | 5 |
YbTi2CdO6F (mp-677010) | 0.4933 | 0.121 | 5 |
NdTi2CdO6F (mp-677732) | 0.5121 | 0.159 | 5 |
EuTi2CdO6F (mp-684730) | 0.5103 | 0.099 | 5 |
NaYbTiNbO6F (mp-684861) | 0.7331 | 0.065 | 6 |
NaEuTiNbO6F (mp-43048) | 0.7030 | 0.021 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 Zr_sv O |
Final Energy/Atom-8.9772 eV |
Corrected Energy-207.1158 eV
Uncorrected energy = -197.4978 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Corrected energy = -207.1158 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)