Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.976 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.087 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2O + Li6TeO6 + Te |
Band Gap2.638 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 190.6 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 178.9 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 280.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 354.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 326.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 245.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 299.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 108.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 27.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 81.7 |
Al (mp-134) | <1 1 0> | <0 0 1> | 163.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 27.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 108.9 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 326.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 190.6 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 178.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 326.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 108.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 326.8 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 163.4 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 268.3 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 268.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 89.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 217.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 163.4 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 89.4 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 108.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 27.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 89.4 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 93.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 1> | 280.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 190.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 178.9 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 178.9 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 354.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 163.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 89.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 54.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 89.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 54.5 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 190.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 190.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 163.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 89.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 326.8 |
C (mp-66) | <1 1 0> | <0 0 1> | 354.0 |
C (mp-66) | <1 1 1> | <0 0 1> | 190.6 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 163.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 81.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 27.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li8BiO6 (mp-754586) | 0.1741 | 0.033 | 3 |
Li8SbS6 (mp-768171) | 0.2284 | 0.060 | 3 |
Li8PbO6 (mp-22538) | 0.1626 | 0.001 | 3 |
Li8WO6 (mp-780046) | 0.2183 | 0.039 | 3 |
Li8ZrO6 (mp-755225) | 0.2211 | 0.001 | 3 |
Li6Mn(FeO3)2 (mp-764386) | 0.5345 | 0.040 | 4 |
Li8VO5F (mp-765837) | 0.6246 | 0.049 | 4 |
K2Th(CuS2)2 (mp-555425) | 0.6054 | 0.013 | 4 |
LiFeCuS2 (mp-755288) | 0.5983 | 0.124 | 4 |
Na2Zr(CuS2)2 (mp-556536) | 0.6891 | 0.000 | 4 |
Mg3As2 (mp-7891) | 0.6237 | 0.018 | 2 |
Hf3N4 (mp-754434) | 0.4485 | 0.074 | 2 |
Zr3N4 (mp-754353) | 0.4443 | 0.051 | 2 |
Pu2O3 (mp-21423) | 0.6214 | 0.073 | 2 |
Th3N4 (mp-467) | 0.4945 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Te O |
Final Energy/Atom-4.9014 eV |
Corrected Energy-77.7351 eV
-77.7351 eV = -73.5214 eV (uncorrected energy) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)