Final Magnetic Moment0.379 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.916 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.084 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu3(PO4)2 + Li2CuP2O7 + CuO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 270.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 135.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 202.9 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 320.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 149.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 160.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 149.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 133.1 |
Te2W (mp-22693) | <1 0 1> | <1 0 1> | 199.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 80.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 240.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 320.0 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 240.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 80.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 320.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 160.0 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 270.6 |
BN (mp-984) | <1 0 1> | <1 0 1> | 199.7 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 320.0 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 270.6 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 160.0 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 240.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 240.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 320.0 |
TeO2 (mp-2125) | <1 1 0> | <1 0 1> | 199.7 |
SiC (mp-7631) | <0 0 1> | <1 0 -1> | 133.1 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 160.0 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 320.0 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 202.9 |
Mg (mp-153) | <1 0 0> | <1 0 -1> | 133.1 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 202.9 |
C (mp-66) | <1 0 0> | <0 1 0> | 202.9 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 135.3 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 -1> | 133.1 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 -1> | 133.1 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 320.0 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 160.0 |
Ni (mp-23) | <1 1 1> | <0 1 0> | 270.6 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 320.0 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 240.0 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 80.0 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 -1> | 266.2 |
SiC (mp-11714) | <0 0 1> | <1 0 -1> | 133.1 |
MoSe2 (mp-1634) | <1 1 1> | <0 1 0> | 270.6 |
Si (mp-149) | <1 0 0> | <0 0 1> | 149.7 |
Au (mp-81) | <1 1 0> | <0 0 1> | 149.7 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 80.0 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 270.6 |
Au (mp-81) | <1 1 1> | <0 1 0> | 270.6 |
C (mp-48) | <0 0 1> | <1 0 0> | 320.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CdGeO3 (mp-2951) | 0.5018 | 0.001 | 3 |
Li2Cr2O7 (mp-770745) | 0.4561 | 0.068 | 3 |
VSiO3 (mp-769952) | 0.4934 | 0.019 | 3 |
Fe3(SiO4)2 (mp-31859) | 0.4977 | 0.172 | 3 |
Fe19(SiO4)12 (mp-775380) | 0.5003 | 0.542 | 3 |
Li2Mn3(PO4)3 (mp-778864) | 0.2508 | 0.192 | 4 |
Li3Ni2(PO4)3 (mp-504123) | 0.2685 | 0.072 | 4 |
Na3Fe2(MoO4)3 (mp-560526) | 0.3245 | 0.220 | 4 |
Na3In2(AsO4)3 (mp-22804) | 0.2927 | 0.000 | 4 |
Li3V2(PO4)3 (mp-540455) | 0.2855 | 0.085 | 4 |
MoO2 (mvc-6944) | 0.7423 | 0.281 | 2 |
Li6MnV3(PO4)6 (mp-764970) | 0.3691 | 0.204 | 5 |
Li6MnV3(PO4)6 (mp-764856) | 0.3753 | 0.168 | 5 |
Li6MnV3(PO4)6 (mp-764485) | 0.3698 | 0.114 | 5 |
Li6MnV3(PO4)6 (mp-764756) | 0.3752 | 0.154 | 5 |
Li6MnV3(PO4)6 (mp-779407) | 0.3673 | 0.122 | 5 |
Li4CrCo2Ni3(PO4)6 (mp-776777) | 0.7054 | 0.086 | 6 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.7034 | 0.080 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.4641 | 0.008 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.6194 | 0.018 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.6796 | 0.778 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv P O |
Final Energy/Atom-6.1905 eV |
Corrected Energy-264.4741 eV
-264.4741 eV = -247.6191 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)