Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.900 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.059 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.33 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaWO4 + Ca3WO6 |
Band Gap3.012 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 199.9 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 70.9 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 175.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 80.0 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 58.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 293.7 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 70.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 235.3 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 264.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 80.0 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 293.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 120.0 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 105.7 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 58.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 212.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 175.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 159.9 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 58.6 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 58.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 239.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 313.7 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 141.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 156.8 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 293.7 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 293.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 199.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 120.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 199.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 159.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 199.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 156.8 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 235.3 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 279.9 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 293.7 |
TePb (mp-19717) | <1 1 1> | <1 1 0> | 293.7 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 88.0 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 235.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 279.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 120.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 359.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 120.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 293.0 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 70.9 |
MoS2 (mp-1434) | <1 1 0> | <0 1 0> | 117.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 199.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 70.9 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 175.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 141.9 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 235.3 |
CdTe (mp-406) | <1 1 1> | <1 1 0> | 293.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaCr2O6 (mvc-13364) | 0.6411 | 0.307 | 3 |
TiNb2O7 (mp-758243) | 0.6237 | 0.048 | 3 |
ZrPbO3 (mp-647557) | 0.6422 | 0.030 | 3 |
TiNb2O7 (mp-759307) | 0.6001 | 0.032 | 3 |
SrMgF4 (mp-1095258) | 0.6336 | 0.025 | 3 |
CuBi(WO4)2 (mp-565192) | 0.6801 | 0.040 | 4 |
NdCu(WO4)2 (mp-504997) | 0.6335 | 0.033 | 4 |
YCu(WO4)2 (mvc-16288) | 0.6713 | 0.030 | 4 |
SrTa2Bi2O9 (mp-23089) | 0.6570 | 0.000 | 4 |
CuBi(WO4)2 (mp-615173) | 0.6812 | 0.040 | 4 |
Nb2O5 (mp-680944) | 0.6105 | 0.036 | 2 |
V3O7 (mp-773443) | 0.6337 | 0.039 | 2 |
Nb2O5 (mp-556048) | 0.6566 | 0.046 | 2 |
Nb12O29 (mp-510554) | 0.6010 | 0.015 | 2 |
Nb12O29 (mp-1470) | 0.6298 | 0.014 | 2 |
Na2LiLa3Ti6O18 (mp-676447) | 0.7420 | 0.043 | 5 |
SrLaTa2(NO)3 (mp-694929) | 0.7261 | 0.020 | 5 |
Hg12SbBr(ClO3)2 (mp-642625) | 0.6398 | 0.031 | 5 |
TiNb2Zn(PbO3)4 (mp-684723) | 0.7160 | 0.058 | 5 |
Na11La7Th2Ti20O60 (mp-686371) | 0.7239 | 0.039 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Ca_sv W_pv O |
Final Energy/Atom-7.1178 eV |
Corrected Energy-259.2190 eV
-259.2190 eV = -227.7692 eV (uncorrected energy) - 17.4040 eV (MP Advanced Correction) - 14.0458 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)