Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.771 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.011 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.77 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2SiO3 + Li2MnSiO4 |
Band Gap3.654 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 314.5 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 74.1 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 314.5 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 134.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 222.4 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 83.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 224.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 89.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 83.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 134.8 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 224.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 166.1 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 90.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 148.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 148.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 83.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 222.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 44.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 166.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 179.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 224.6 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 166.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 134.8 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 224.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 224.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 148.2 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 269.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 134.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 222.4 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 296.5 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 269.6 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 222.4 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 44.9 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 -1> | 166.1 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 134.8 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 249.1 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 224.6 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 148.2 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 148.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 296.5 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 166.1 |
Te2Mo (mp-602) | <1 0 1> | <1 0 1> | 270.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 134.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 224.6 |
BN (mp-984) | <1 0 0> | <1 0 1> | 270.5 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 224.6 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 89.9 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 296.5 |
BN (mp-984) | <1 0 1> | <1 0 0> | 224.6 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 224.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaFeO2 (mp-24939) | 0.3912 | 0.050 | 3 |
NaGaO2 (mp-3338) | 0.4028 | 0.000 | 3 |
Li3PS4 (mp-1097036) | 0.3993 | 0.016 | 3 |
Li2SiO3 (mp-5012) | 0.2787 | 0.000 | 3 |
NaFeO2 (mp-566778) | 0.3875 | 0.050 | 3 |
Li4Si2NiO7 (mp-767687) | 0.2051 | 0.069 | 4 |
Li4CuSi2O7 (mp-765980) | 0.2151 | 0.049 | 4 |
Li4FeSi2O7 (mp-761968) | 0.1063 | 0.010 | 4 |
Li3AlSiO5 (mp-1020023) | 0.2429 | 0.000 | 4 |
Li2PNO2 (mp-1020019) | 0.2444 | 0.000 | 4 |
CdP2 (mp-913) | 0.5979 | 0.000 | 2 |
ZnP2 (mp-680550) | 0.7218 | 0.190 | 2 |
Si3H (mp-995193) | 0.7202 | 0.032 | 2 |
CdP2 (mp-402) | 0.7234 | 0.001 | 2 |
CdP2 (mp-12112) | 0.5971 | 0.000 | 2 |
Si (mp-1095269) | 0.7457 | 0.094 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Si O |
Final Energy/Atom-6.7480 eV |
Corrected Energy-404.2733 eV
-404.2733 eV = -377.8858 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)