Final Magnetic Moment0.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.487 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.233 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi4P2O7 + VP + Li3PO4 + VPO4 |
Band Gap3.013 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 329.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 319.7 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 283.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 319.7 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 279.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 274.1 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 310.9 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 101.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 228.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 228.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 283.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 319.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 182.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 319.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 -1> | 213.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 319.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 310.9 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 207.3 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 279.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 310.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 283.9 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 283.9 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 197.8 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 319.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 319.7 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 207.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 319.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 319.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 245.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 274.1 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 329.7 |
YVO4 (mp-19133) | <1 0 1> | <1 -1 -1> | 218.4 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 201.9 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 329.7 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 189.3 |
BN (mp-984) | <0 0 1> | <1 1 -1> | 213.1 |
BN (mp-984) | <1 1 1> | <0 0 1> | 137.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 228.4 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 274.1 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 189.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 319.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 310.9 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 319.7 |
LiNbO3 (mp-3731) | <1 1 1> | <0 1 0> | 259.1 |
MoS2 (mp-1434) | <1 0 0> | <1 1 1> | 201.9 |
BN (mp-984) | <1 0 0> | <0 1 0> | 155.5 |
BN (mp-984) | <1 0 1> | <0 1 1> | 197.8 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 279.6 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 -1> | 216.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 182.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr2PO5 (mp-770913) | 0.6559 | 0.049 | 3 |
Cr4P2O9 (mp-773396) | 0.6875 | 0.230 | 3 |
Na2Ge2O5 (mp-780053) | 0.6240 | 0.020 | 3 |
Na4P2O7 (mp-27579) | 0.6998 | 0.000 | 3 |
Na2Si2O5 (mp-556423) | 0.6971 | 0.000 | 3 |
Li2FeP2O7 (mp-850262) | 0.5119 | 0.000 | 4 |
Li2NiP2O7 (mp-764152) | 0.5101 | 0.189 | 4 |
Li5MnP3O11 (mp-761571) | 0.1614 | 0.284 | 4 |
Li5FeP3O11 (mp-761453) | 0.1982 | 0.129 | 4 |
Li5NiP3O11 (mp-861091) | 0.2128 | 0.074 | 4 |
Li7MnP4O14F (mp-762708) | 0.3865 | 0.151 | 5 |
Li7FeP4O14F (mp-762690) | 0.3916 | 0.126 | 5 |
Li7CuAs4ClO14 (mp-769204) | 0.6790 | 0.074 | 5 |
CuAg7As4ClO14 (mp-653450) | 0.6390 | 0.015 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-6.4812 eV |
Corrected Energy-277.7609 eV
Uncorrected energy = -259.2469 eV
Composition-based energy adjustment (-0.687 eV/atom x 22.0 atoms) = -15.1140 eV
Composition-based energy adjustment (-1.700 eV/atom x 2.0 atoms) = -3.4000 eV
Corrected energy = -277.7609 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)