Final Magnetic Moment16.877 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.379 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.006 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi19Ni23O42 + LiNiO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 139.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 181.1 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 224.6 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 324.5 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 101.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 213.2 |
AlN (mp-661) | <0 0 1> | <1 -1 -1> | 288.4 |
AlN (mp-661) | <1 1 1> | <1 -1 -1> | 288.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 301.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 241.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 110.2 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 203.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 241.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 301.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 241.5 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 259.6 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 149.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 -1> | 219.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 181.1 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 324.5 |
SiO2 (mp-6930) | <1 1 1> | <0 1 -1> | 219.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 224.6 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 203.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 224.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 181.1 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 -1> | 288.4 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 110.2 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 203.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 259.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 224.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 224.6 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 301.9 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 259.6 |
LiF (mp-1138) | <1 1 1> | <0 1 -1> | 146.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 241.5 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 278.2 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 324.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 120.8 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 220.4 |
Ag (mp-124) | <1 1 1> | <0 1 -1> | 146.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 101.8 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 101.8 |
BN (mp-984) | <1 0 0> | <0 1 -1> | 292.4 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 224.6 |
MoS2 (mp-1434) | <1 0 0> | <1 -1 1> | 199.7 |
Al (mp-134) | <1 1 1> | <0 1 -1> | 146.2 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 224.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 129.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 -1 0> | 231.6 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 -1> | 224.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4Ni5O9 (mp-767950) | 0.0951 | 0.051 | 3 |
Li19Ni23O42 (mp-698842) | 0.1399 | 0.000 | 3 |
Li13Ni9O22 (mp-769473) | 0.1640 | 0.008 | 3 |
Li13Ni15O28 (mp-769435) | 0.1017 | 0.005 | 3 |
Li7Ni5O12 (mp-761436) | 0.1374 | 0.022 | 3 |
Li5Co5(NiO6)2 (mp-766793) | 0.1227 | 0.257 | 4 |
Li4Ni3O6F (mp-764986) | 0.1455 | 0.063 | 4 |
Li5Mn(Ni2O5)2 (mp-853151) | 0.1422 | 0.074 | 4 |
Li4FeNi3O8 (mp-765712) | 0.1409 | 0.180 | 4 |
Li5Ni5O9F (mp-764733) | 0.1458 | 0.038 | 4 |
Te2Au (mp-1662) | 0.3658 | 0.018 | 2 |
NaTe3 (mp-28478) | 0.4011 | 0.000 | 2 |
LiTe3 (mp-27466) | 0.3196 | 0.009 | 2 |
Sb2Te3 (mp-1080789) | 0.4196 | 0.129 | 2 |
Te2Au (mp-567525) | 0.3757 | 0.018 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.4319 | 0.005 | 5 |
Hg (mp-982872) | 0.6235 | 0.020 | 1 |
Sb (mp-632286) | 0.4591 | 0.059 | 1 |
Bi (mp-23152) | 0.6174 | 0.000 | 1 |
Te (mp-570459) | 0.4421 | 0.044 | 1 |
Te (mp-105) | 0.5260 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv O |
Final Energy/Atom-4.9133 eV |
Corrected Energy-327.2691 eV
-327.2691 eV = -275.1450 eV (uncorrected energy) - 32.4600 eV (MP Advanced Correction) - 19.6641 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)