Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.581 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.044 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Si2O5 + Fe2O3 |
Band Gap3.154 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP213 [198] |
HallP 2ac 2ab 3 |
Point Group23 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 1> | 276.1 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 225.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 265.7 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 225.4 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 150.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 265.7 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 276.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 212.5 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 150.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 212.5 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 265.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 53.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 225.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 212.5 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 75.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 159.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 265.7 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 276.1 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 276.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 265.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 276.1 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 265.7 |
Al (mp-134) | <1 0 0> | <1 0 0> | 212.5 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 265.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 265.7 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 225.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 212.5 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 225.4 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 276.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 265.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 225.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 265.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 212.5 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 225.4 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 225.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 212.5 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 318.8 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 92.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 106.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 265.7 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 225.4 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 225.4 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 92.0 |
BN (mp-984) | <1 0 0> | <1 0 0> | 159.4 |
BN (mp-984) | <1 1 0> | <1 1 1> | 276.1 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 265.7 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 225.4 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 225.4 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 265.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 265.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | -0.11131 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.11131 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.11131 |
Piezoelectric Modulus ‖eij‖max0.11131 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.04 | 0.00 | 0.00 |
0.00 | 3.04 | 0.00 |
0.00 | 0.00 | 3.04 |
Dielectric Tensor εij (total) |
||
---|---|---|
6.85 | 0.00 | 0.00 |
0.00 | 6.85 | 0.00 |
0.00 | 0.00 | 6.85 |
Polycrystalline dielectric constant
εpoly∞
3.04
|
Polycrystalline dielectric constant
εpoly
6.85
|
Refractive Index n1.74 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCN2 (mp-29826) | 0.6873 | 0.000 | 3 |
Zn4B2O7 (mp-686042) | 0.7242 | 0.089 | 3 |
Si2CN4 (mp-30161) | 0.6551 | 0.000 | 3 |
BHO2 (mp-721851) | 0.6462 | 0.006 | 3 |
LiVSiO4 (mp-767784) | 0.0879 | 0.084 | 4 |
LiFeSiO4 (mp-763740) | 0.2878 | 0.047 | 4 |
LiFePO4 (mp-766761) | 0.2458 | 0.091 | 4 |
LiMnPO4 (mp-766734) | 0.2700 | 0.100 | 4 |
LiVSiO4 (mp-767097) | 0.2713 | 0.079 | 4 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Si O |
Final Energy/Atom-6.8745 eV |
Corrected Energy-214.6555 eV
-214.6555 eV = -192.4869 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)