Final Magnetic Moment5.006 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.853 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.073 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Si2O5 + Fe2O3 + SiO2 |
Band Gap3.182 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 294.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 109.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 147.4 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 236.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 294.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 134.5 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 236.2 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 240.9 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 236.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 221.1 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 134.5 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 314.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 294.9 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 218.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 221.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 73.7 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 107.8 |
BN (mp-984) | <0 0 1> | <1 0 1> | 109.0 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 236.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 294.9 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 294.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 236.2 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 1> | 218.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 314.9 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 215.7 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 240.9 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 240.9 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 294.9 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 218.0 |
C (mp-66) | <1 1 0> | <0 1 1> | 107.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 221.1 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 236.2 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 1> | 218.0 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 73.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 73.7 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 294.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 221.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 73.7 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 157.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 73.7 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 157.5 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 240.9 |
PbSe (mp-2201) | <1 1 0> | <1 0 1> | 109.0 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 236.2 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 1> | 215.7 |
NdGaO3 (mp-3196) | <1 0 1> | <0 1 0> | 157.5 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 294.9 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 73.7 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 314.9 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 236.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2PbO4 (mp-21892) | 0.4868 | 0.000 | 3 |
SrAl2O4 (mp-36775) | 0.6160 | 0.012 | 3 |
Na2Si3O7 (mp-556198) | 0.5082 | 0.016 | 3 |
Mn2Si4O11 (mp-768088) | 0.6078 | 0.090 | 3 |
SrAl2O4 (mp-3094) | 0.5827 | 0.000 | 3 |
Li2FeP2O7 (mp-765934) | 0.5770 | 0.081 | 4 |
Li2CoP2O7 (mp-761663) | 0.5618 | 0.072 | 4 |
KAl(SiO3)2 (mp-554433) | 0.5806 | 0.004 | 4 |
ZnSn(GeO3)2 (mvc-8156) | 0.5540 | 0.096 | 4 |
BeAgPO4 (mp-15919) | 0.5735 | 0.000 | 4 |
Zn2P2HNO8 (mp-707891) | 0.7158 | 0.533 | 5 |
Na8Be3Si9(ClO12)2 (mp-40201) | 0.6822 | 0.037 | 5 |
RbZn2P2HO8 (mp-24683) | 0.7486 | 0.000 | 5 |
Na4BeAlSi4ClO12 (mp-42508) | 0.6540 | 0.046 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Si O |
Final Energy/Atom-7.3057 eV |
Corrected Energy-413.3028 eV
-413.3028 eV = -379.8975 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)