Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.893 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.033 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Si2O5 + Fe2O3 + SiO2 |
Band Gap3.336 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 209.6 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 256.1 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 311.4 |
AlN (mp-661) | <1 0 0> | <1 -1 0> | 299.6 |
AlN (mp-661) | <1 0 1> | <1 1 -1> | 272.4 |
AlN (mp-661) | <1 1 0> | <1 -1 0> | 299.6 |
AlN (mp-661) | <1 1 1> | <1 -1 1> | 231.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 -1> | 252.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 -1> | 272.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 311.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 -1> | 281.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 314.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 157.2 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 256.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 162.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 311.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 262.0 |
CdS (mp-672) | <1 1 1> | <1 1 -1> | 204.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 157.2 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 314.4 |
BaF2 (mp-1029) | <1 0 0> | <0 1 -1> | 202.0 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 251.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 207.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 270.5 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 155.7 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 259.5 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 337.7 |
YVO4 (mp-19133) | <1 0 1> | <0 1 -1> | 202.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 262.0 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 279.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 270.5 |
Ag (mp-124) | <1 1 1> | <1 0 -1> | 337.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 259.5 |
SiO2 (mp-6930) | <1 0 0> | <1 1 -1> | 136.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 -1> | 252.5 |
KCl (mp-23193) | <1 0 0> | <0 1 -1> | 202.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 271.3 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 271.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 157.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 -1> | 252.5 |
BN (mp-984) | <1 0 0> | <0 1 -1> | 151.5 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 281.4 |
BN (mp-984) | <1 1 0> | <1 0 0> | 104.8 |
InAs (mp-20305) | <1 0 0> | <0 1 -1> | 202.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 157.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 262.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 311.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 -1> | 252.5 |
Bi2Se3 (mp-541837) | <1 0 1> | <0 1 0> | 259.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 162.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2Ti2O5 (mp-781948) | 0.5002 | 0.013 | 3 |
Na2V2O5 (mp-779376) | 0.5587 | 0.191 | 3 |
Li2Si2O5 (mp-3552) | 0.4895 | 0.006 | 3 |
Li2Si2O5 (mp-4117) | 0.5908 | 0.000 | 3 |
Li2Si3O7 (mp-555899) | 0.5162 | 0.002 | 3 |
LiVSi3O8 (mp-767324) | 0.5296 | 0.053 | 4 |
Li2Fe2Si8O19 (mp-765416) | 0.4919 | 0.175 | 4 |
LiCo2(PO4)2 (mp-769426) | 0.5364 | 0.404 | 4 |
LiFe2(SiO4)2 (mp-762762) | 0.5125 | 0.115 | 4 |
LiFeSi3O8 (mp-761820) | 0.3775 | 0.221 | 4 |
SiO2 (mp-557723) | 0.7389 | 0.275 | 2 |
P3N5 (mp-567907) | 0.6920 | 0.000 | 2 |
Ca5Al11TlSi13O48 (mp-703276) | 0.6182 | 0.177 | 5 |
NaLi2Al3(SiO4)3 (mp-693857) | 0.5499 | 0.109 | 5 |
Na2Li5Al7Si29O72 (mp-694958) | 0.7027 | 0.054 | 5 |
K6Al11Si13Ag5O48 (mp-686585) | 0.7225 | 0.171 | 5 |
Na8Al11Si13(AgO16)3 (mp-690919) | 0.7050 | 0.213 | 5 |
Na3CaAl4Si8ClO24 (mp-684921) | 0.7448 | 0.008 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Si O |
Final Energy/Atom-7.3462 eV |
Corrected Energy-207.7031 eV
-207.7031 eV = -191.0004 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)