Final Magnetic Moment0.997 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.882 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.092 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.42 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2VSiO5 + SiO2 |
Band Gap2.106 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 170.1 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 297.6 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 203.9 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 126.2 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 297.6 |
BN (mp-984) | <1 0 0> | <0 1 0> | 255.1 |
BN (mp-984) | <1 0 1> | <0 0 1> | 297.6 |
BN (mp-984) | <1 1 0> | <0 1 0> | 170.1 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 102.0 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 126.2 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 1> | 226.0 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 102.0 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 85.0 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 203.9 |
Al (mp-134) | <1 1 0> | <1 0 1> | 252.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 170.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 102.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 252.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 297.6 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 126.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 252.4 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 170.1 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 223.2 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 297.6 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 132.8 |
SiC (mp-7631) | <1 1 0> | <1 0 1> | 252.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 255.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 85.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 223.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 223.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 255.1 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 1> | 226.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 223.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 252.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 223.2 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 255.1 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 223.2 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 102.0 |
TiO2 (mp-2657) | <1 1 1> | <1 1 0> | 265.5 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 170.1 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 297.6 |
C (mp-66) | <1 0 0> | <0 1 0> | 255.1 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 255.1 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 0> | 85.0 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 223.2 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 255.1 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 148.8 |
LaF3 (mp-905) | <1 1 0> | <1 1 0> | 265.5 |
GaP (mp-2490) | <1 1 0> | <0 1 0> | 85.0 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 148.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni4P4O15 (mp-585202) | 0.5666 | 0.059 | 3 |
Sn2Ge2O7 (mp-768877) | 0.5312 | 0.059 | 3 |
MgSiO3 (mp-1020124) | 0.5948 | 0.028 | 3 |
MgSiO3 (mp-1020123) | 0.5801 | 0.039 | 3 |
Ni4P4O15 (mp-705427) | 0.5718 | 0.059 | 3 |
Mg3Si4(MoO7)2 (mvc-5195) | 0.3928 | 0.224 | 4 |
Zn3Fe2(Si2O7)2 (mvc-4877) | 0.3536 | 0.174 | 4 |
Zn3Cr2(Si2O7)2 (mvc-4831) | 0.3944 | 0.122 | 4 |
V2Zn3(Si2O7)2 (mvc-4629) | 0.3746 | 0.242 | 4 |
Ti2Zn3(Si2O7)2 (mvc-4488) | 0.3726 | 0.147 | 4 |
FeO2 (mvc-11999) | 0.6759 | 0.720 | 2 |
CrO2 (mvc-11581) | 0.7258 | 0.166 | 2 |
NiO2 (mvc-6939) | 0.7484 | 0.456 | 2 |
CoO2 (mvc-6933) | 0.7429 | 0.254 | 2 |
Li2VCr(P2O7)2 (mp-765058) | 0.4750 | 0.012 | 5 |
Li2VCr(P2O7)2 (mp-763864) | 0.4752 | 0.012 | 5 |
Li2VCr(P2O7)2 (mp-764248) | 0.4737 | 0.000 | 5 |
Li2VCr(P2O7)2 (mp-764239) | 0.4708 | 0.000 | 5 |
Li2VCr(P2O7)2 (mp-763868) | 0.4757 | 0.012 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.7447 | 0.257 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.6912 | 0.331 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6031 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Si O |
Final Energy/Atom-7.2627 eV |
Corrected Energy-467.7712 eV
-467.7712 eV = -435.7608 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)