Final Magnetic Moment4.898 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.230 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.059 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoO2 + Co3O4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 326.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 195.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 261.2 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 326.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 326.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 326.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 65.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 65.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 92.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 65.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 92.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 113.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 326.5 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 113.1 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 326.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 195.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 65.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 92.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 326.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 277.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 130.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 92.4 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 326.5 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 261.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 65.3 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 92.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 261.2 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 184.7 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 277.1 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 113.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 195.9 |
BN (mp-984) | <1 0 1> | <1 1 0> | 184.7 |
Al (mp-134) | <1 0 0> | <1 0 0> | 65.3 |
Al (mp-134) | <1 1 0> | <1 1 0> | 92.4 |
Al (mp-134) | <1 1 1> | <1 1 1> | 113.1 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 130.6 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 184.7 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 277.1 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 277.1 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 195.9 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 326.5 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 326.5 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 277.1 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 326.5 |
C (mp-66) | <1 0 0> | <1 0 0> | 326.5 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 130.6 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 92.4 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 326.5 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 65.3 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 184.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ScAlCO (mp-972937) | 0.6444 | 0.000 | 4 |
Li2Fe3O3F5 (mp-849525) | 0.5566 | 0.097 | 4 |
Li7Mn10Cr6O32 (mp-769505) | 0.4727 | 0.000 | 4 |
LiMn3CrO8 (mp-773299) | 0.1298 | 0.007 | 4 |
Li3Mn5Cr3O16 (mp-775496) | 0.3271 | 0.000 | 4 |
In2S3 (mp-22216) | 0.6587 | 0.000 | 2 |
Mn21O40 (mp-767941) | 0.5377 | 0.055 | 2 |
Mn21O40 (mp-849596) | 0.6161 | 0.043 | 2 |
Co21O40 (mp-851287) | 0.5578 | 0.066 | 2 |
Co2S3 (mp-684732) | 0.3831 | 0.028 | 2 |
LiMn4O8 (mp-35530) | 0.0579 | 0.038 | 3 |
Na3Ti8O16 (mp-760062) | 0.3215 | 0.042 | 3 |
Cr10Fe5O24 (mp-771184) | 0.1942 | 0.102 | 3 |
Mg2Mn3O8 (mp-771763) | 0.2400 | 0.040 | 3 |
Cr3(FeO4)2 (mp-771791) | 0.2169 | 0.096 | 3 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points8 |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Co O |
Final Energy/Atom-5.8485 eV |
Corrected Energy-91.0189 eV
-91.0189 eV = -76.0306 eV (uncorrected energy) - 9.3700 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)