Final Magnetic Moment5.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.567 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.078 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.30 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnPO4 |
Band Gap3.274 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPna21 [33] |
HallP 2c 2n |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <0 0 1> | 143.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 238.8 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 122.3 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 244.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 238.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 191.1 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 244.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 95.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 238.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 95.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 238.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 167.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 225.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 334.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 112.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 112.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 238.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 334.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 225.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 112.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 191.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 167.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 47.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 95.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 238.8 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 173.8 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 173.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 334.4 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 286.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 191.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 191.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 286.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 238.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 143.3 |
MoS2 (mp-1434) | <1 1 0> | <0 1 1> | 122.3 |
MoS2 (mp-1434) | <1 1 1> | <0 0 1> | 238.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 334.4 |
Al (mp-134) | <1 1 1> | <0 1 0> | 112.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 143.3 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 95.5 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 143.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 1> | 173.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 143.3 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 238.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 238.8 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 238.8 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 143.3 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 225.2 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 143.3 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 225.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2Ti2O5 (mp-779477) | 0.5110 | 0.026 | 3 |
Mn2PO5 (mp-770541) | 0.5674 | 0.059 | 3 |
Na2V2O5 (mp-764595) | 0.4943 | 0.138 | 3 |
Cd3(PO4)2 (mp-680761) | 0.5425 | 0.000 | 3 |
Cd3(AsO4)2 (mp-13602) | 0.5858 | 0.000 | 3 |
LiV4(PO4)3 (mp-763404) | 0.4536 | 0.282 | 4 |
LiMnPO4 (mp-861688) | 0.3603 | 0.819 | 4 |
LiCrPO4 (mp-761399) | 0.4258 | 0.287 | 4 |
LiNiPO4 (mp-766636) | 0.3517 | 0.098 | 4 |
LiCoPO4 (mp-761753) | 0.4406 | 0.141 | 4 |
Li3CrPCO7 (mp-771604) | 0.6342 | 0.197 | 5 |
Li3ZnPCO7 (mp-772753) | 0.6399 | 0.046 | 5 |
Li3CuAsCO7 (mp-768589) | 0.6336 | 0.067 | 5 |
Sr2AlGaW2O7 (mvc-16391) | 0.5819 | 0.510 | 5 |
Li2PWO4F (mp-25728) | 0.5094 | 0.352 | 5 |
Li12Mn3CrP4(CO7)4 (mp-767734) | 0.6971 | 0.056 | 6 |
Li6MnCrP2(CO7)2 (mp-767287) | 0.6914 | 0.062 | 6 |
Na2LiCaVP2O9 (mp-763838) | 0.6477 | 0.111 | 6 |
Na3LiMnBPO7 (mp-763842) | 0.6715 | 0.211 | 6 |
NaLi5Mn2P2(CO7)2 (mp-773772) | 0.7116 | 0.067 | 6 |
Explore more synthesis descriptions for materials of composition LiMnPO4.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-7.1074 eV |
Corrected Energy-650.0143 eV
Uncorrected energy = -597.0223 eV
Composition-based energy adjustment (-0.687 eV/atom x 48.0 atoms) = -32.9760 eV
Composition-based energy adjustment (-1.668 eV/atom x 12.0 atoms) = -20.0160 eV
Corrected energy = -650.0143 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)