Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.619 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.060 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.97 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn2P2O7 + Li4P2O7 |
Band Gap3.293 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <0 0 1> | 187.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 93.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 170.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 177.8 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 280.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 148.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 280.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 93.5 |
BN (mp-984) | <0 0 1> | <0 1 0> | 256.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 280.5 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 187.0 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 256.2 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 256.2 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 93.5 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 187.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 280.5 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 187.0 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 280.5 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 93.5 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 280.5 |
Au (mp-81) | <1 1 0> | <1 0 0> | 148.2 |
WS2 (mp-224) | <1 0 0> | <1 0 1> | 177.8 |
C (mp-48) | <1 0 1> | <0 1 0> | 256.2 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 256.2 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 280.5 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 280.5 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 280.5 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 280.5 |
ZrO2 (mp-2858) | <1 1 1> | <0 1 1> | 253.3 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 187.0 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 280.5 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 280.5 |
LiAlO2 (mp-3427) | <1 1 0> | <0 0 1> | 93.5 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 280.5 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 187.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe4(PO4)3 (mp-704185) | 0.5976 | 0.097 | 3 |
CuPO3 (mp-766856) | 0.5893 | 0.090 | 3 |
Ag7P3S11 (mp-683910) | 0.5336 | 0.019 | 3 |
Li4P2O7 (mp-1020666) | 0.4930 | 0.620 | 3 |
LiBeH3 (mp-24818) | 0.4598 | 0.006 | 3 |
Li2VP2O7 (mp-767710) | 0.2400 | 0.224 | 4 |
LiCuPO4 (mp-673128) | 0.4602 | 0.129 | 4 |
Li3Fe(PO4)2 (mp-31776) | 0.4627 | 0.027 | 4 |
Li3Ni(PO4)2 (mp-32371) | 0.4489 | 0.085 | 4 |
Li3Cu(PO4)2 (mp-26224) | 0.4155 | 0.050 | 4 |
Na4Al3Ge3NO15 (mp-677474) | 0.7431 | 0.177 | 5 |
Na4Al3Ge3NO14 (mp-720104) | 0.7398 | 0.000 | 5 |
NaLi2B(PO4)2 (mp-1020646) | 0.7298 | 0.000 | 5 |
KMg3AlSi3(O5F)2 (mp-684841) | 0.7450 | 0.230 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-6.9399 eV |
Corrected Energy-359.5014 eV
-359.5014 eV = -333.1139 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)