Final Magnetic Moment2.936 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.507 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnO2 + LiPO3 |
Band Gap0.404 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 81.3 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 146.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 162.7 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 189.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 162.7 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 171.4 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 145.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 81.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 162.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 81.3 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 171.4 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 171.4 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 122.0 |
TePb (mp-19717) | <1 1 1> | <1 0 1> | 146.7 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 162.7 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 81.3 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 162.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 81.3 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 189.7 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 162.7 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 162.7 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 162.7 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 244.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 162.7 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 1> | 146.7 |
YAlO3 (mp-3792) | <1 0 1> | <0 1 1> | 145.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 162.7 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 162.7 |
Mg (mp-153) | <1 0 1> | <1 1 0> | 171.4 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 244.1 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 122.0 |
MgF2 (mp-1249) | <1 1 1> | <0 1 0> | 120.3 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 162.7 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 162.7 |
LiAlO2 (mp-3427) | <1 1 0> | <1 1 1> | 189.7 |
Fe2O3 (mp-24972) | <1 1 0> | <0 1 0> | 120.3 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 162.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TiPN3 (mp-989624) | 0.3953 | 0.015 | 3 |
VGeO3 (mp-769968) | 0.3691 | 0.038 | 3 |
VSiO3 (mp-769952) | 0.3598 | 0.019 | 3 |
CoGeO3 (mp-24885) | 0.3924 | 0.063 | 3 |
CoGeO3 (mp-561981) | 0.3906 | 0.063 | 3 |
Li2Fe(SO4)2 (mp-849220) | 0.3509 | 0.178 | 4 |
Li2Fe(PO4)2 (mp-761516) | 0.1303 | 0.179 | 4 |
Li2Co(SO4)2 (mp-853229) | 0.3111 | 0.071 | 4 |
Li2Ni(SO4)2 (mp-578763) | 0.3107 | 0.051 | 4 |
ZnCrSiO5 (mvc-3237) | 0.3591 | 0.091 | 4 |
CrO2 (mvc-11581) | 0.6434 | 0.166 | 2 |
VO2 (mp-777469) | 0.6113 | 0.038 | 2 |
VO2 (mvc-6918) | 0.5995 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.6115 | 0.281 | 2 |
Fe5O8 (mp-543082) | 0.6270 | 0.163 | 2 |
LiFeSO4F (mp-943492) | 0.4931 | 0.007 | 5 |
LiMnSO4F (mp-942702) | 0.4905 | 0.012 | 5 |
LiCoSO4F (mp-942701) | 0.4858 | 0.006 | 5 |
LiNiSO4F (mp-942700) | 0.4634 | 0.001 | 5 |
LiAlPO4F (mp-41795) | 0.4097 | 0.009 | 5 |
Ca5TaTi3Al(SiO5)5 (mp-720394) | 0.7089 | 0.000 | 6 |
NaCa4Ti4Nb(SiO5)5 (mp-720204) | 0.7108 | 0.073 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.5189 | 0.008 | 6 |
Mn4Si4SnB2(HO9)2 (mp-743890) | 0.6974 | 0.000 | 6 |
Ca5Ti3NbAl(SiO5)5 (mp-720340) | 0.6895 | 0.007 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-6.8219 eV |
Corrected Energy-767.8694 eV
-767.8694 eV = -709.4761 eV (uncorrected energy) - 44.9466 eV (MP Anion Correction) - 13.4468 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)