Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.643 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVPO4 + LiMnPO4 |
Band Gap2.500 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 177.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 206.5 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 233.7 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 71.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 324.5 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 252.1 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 246.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 213.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 285.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 201.7 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 262.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 262.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 354.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 259.6 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 164.4 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 206.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 64.9 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 194.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 324.5 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 201.7 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 201.7 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 324.5 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 201.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 236.0 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 265.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 354.0 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 201.7 |
MoS2 (mp-1434) | <1 0 1> | <0 1 0> | 201.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 236.0 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 324.5 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 262.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 118.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 213.9 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 265.5 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 194.7 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 265.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 236.0 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 285.2 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 174.7 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 87.3 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 1> | 292.1 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 129.8 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 64.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 236.0 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 252.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 201.7 |
C (mp-66) | <1 1 0> | <1 1 0> | 164.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 1 0> | 246.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 265.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 246.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V2SiO4 (mp-772381) | 0.2128 | 0.000 | 3 |
Mn2SiO4 (mp-18928) | 0.1896 | 0.000 | 3 |
Na2BeF4 (mp-3318) | 0.2825 | 0.000 | 3 |
Ca2GeO4 (mp-560647) | 0.2394 | 0.000 | 3 |
Ca2SiO4 (mp-4481) | 0.2033 | 0.000 | 3 |
LiMnPO4 (mp-18997) | 0.0758 | 0.000 | 4 |
LiFePO4 (mp-19017) | 0.1475 | 0.000 | 4 |
LiMgPO4 (mp-9625) | 0.1493 | 0.000 | 4 |
LiVPO4 (mp-25637) | 0.0703 | 0.012 | 4 |
LiTiPO4 (mp-504106) | 0.1382 | 0.346 | 4 |
Fe3S4 (mp-21515) | 0.6841 | 0.197 | 2 |
Fe3S4 (mp-850016) | 0.6882 | 0.144 | 2 |
Cr3N4 (mp-1014379) | 0.6650 | 0.105 | 2 |
Mn3N4 (mp-1080204) | 0.6732 | 0.172 | 2 |
Cr3N4 (mp-1014358) | 0.5809 | 0.227 | 2 |
Li16Mn15Fe(PO4)16 (mp-850169) | 0.0792 | 0.000 | 5 |
Li4MnV3(PO4)4 (mp-761410) | 0.0549 | 0.006 | 5 |
Li4Mn3V(PO4)4 (mp-761418) | 0.0692 | 0.003 | 5 |
Li2VFe(PO4)2 (mp-861602) | 0.0665 | 0.005 | 5 |
Li4TiMn3(PO4)4 (mp-767296) | 0.0719 | 0.081 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.1324 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.1266 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.1278 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.1169 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764867) | 0.1308 | 0.031 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv V_pv P O |
Final Energy/Atom-7.1784 eV |
Corrected Energy-218.9585 eV
-218.9585 eV = -200.9962 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 6.7257 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)