Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.963 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.054 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn7SiO12 + Li5Mn7O16 + Li2Si2O5 + SiO2 |
Band Gap1.069 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 311.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 156.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 234.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 164.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 311.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 234.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 234.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 311.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 234.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 234.0 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 143.0 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 239.6 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 188.4 |
BN (mp-984) | <1 1 1> | <0 0 1> | 234.0 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 239.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 234.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 311.9 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 311.9 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 188.4 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 234.0 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 188.4 |
SiC (mp-7631) | <1 1 0> | <0 1 0> | 239.6 |
SiC (mp-7631) | <1 1 1> | <0 1 0> | 239.6 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 234.0 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 0> | 239.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 311.9 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 1> | 143.0 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 1> | 164.9 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 311.9 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 311.9 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 1> | 164.9 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 311.9 |
LaF3 (mp-905) | <1 1 0> | <1 1 0> | 188.4 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 156.0 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 311.9 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 311.9 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 311.9 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 234.0 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 1> | 164.9 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 234.0 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 239.6 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 234.0 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 311.9 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 1> | 164.9 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 1> | 143.0 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 311.9 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 156.0 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 311.9 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 234.0 |
Ga2O3 (mp-886) | <1 0 1> | <1 1 0> | 188.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sn2Ge2O7 (mp-768877) | 0.5963 | 0.039 | 3 |
Cr4Si4O13 (mp-768078) | 0.6428 | 0.079 | 3 |
Ge2MoO6 (mvc-8403) | 0.6434 | 0.087 | 3 |
Fe(GeO3)2 (mvc-9284) | 0.6309 | 0.127 | 3 |
Mn5(P3O11)2 (mp-31954) | 0.5970 | 0.028 | 3 |
Li3Ti(Si2O5)3 (mp-757542) | 0.2262 | 0.055 | 4 |
Li3Cr(Si2O5)3 (mp-766678) | 0.2505 | 0.038 | 4 |
Li3Fe(Si2O5)3 (mp-761764) | 0.1132 | 0.040 | 4 |
Li3V(Si2O5)3 (mp-761583) | 0.2545 | 0.039 | 4 |
Zn3Co2(Si2O7)2 (mvc-5029) | 0.4820 | 0.133 | 4 |
LiCo2P4H3O16 (mp-762653) | 0.7262 | 0.141 | 5 |
LiFeP2HO8 (mp-762277) | 0.6945 | 0.072 | 5 |
Li3MnV(P2O7)2 (mp-850951) | 0.7014 | 0.000 | 5 |
Li3VCr(P2O7)2 (mp-765133) | 0.7035 | 0.020 | 5 |
Li2V3P4H4O19 (mp-850740) | 0.7140 | 0.059 | 5 |
LiMnVP2(O4F)2 (mp-778336) | 0.7381 | 0.002 | 6 |
Na3Mg4CrSi8(O11F)2 (mp-743787) | 0.7041 | 0.709 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Si O |
Final Energy/Atom-7.3408 eV |
Corrected Energy-782.9413 eV
-782.9413 eV = -734.0805 eV (uncorrected energy) - 42.1374 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)