Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.597 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.048 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnPO4 |
Band Gap3.410 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP61 [169] |
HallP 61 |
Point Group6 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 250.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 250.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 167.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 250.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 83.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 83.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 250.9 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 167.3 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 167.3 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 250.9 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 250.9 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 167.3 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 83.6 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 83.6 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 167.3 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 250.9 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 250.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cu4As2O9 (mp-559159) | 0.5423 | 0.030 | 3 |
Na2Ge2O5 (mp-772811) | 0.6277 | 0.019 | 3 |
MgSiO3 (mp-657336) | 0.6168 | 0.306 | 3 |
Zn4As2O9 (mp-29437) | 0.6197 | 0.008 | 3 |
Cu4P2O9 (mp-5169) | 0.5901 | 0.034 | 3 |
LiCuPO4 (mp-758897) | 0.4366 | 0.077 | 4 |
LiNiPO4 (mp-851065) | 0.3401 | 0.113 | 4 |
Li3Mn(PO4)2 (mp-761596) | 0.3811 | 0.051 | 4 |
LiCrPO4 (mp-773992) | 0.3955 | 0.345 | 4 |
LiCoPO4 (mp-762014) | 0.3348 | 0.113 | 4 |
LiMnPO4F (mp-762683) | 0.5835 | 0.211 | 5 |
Li4TiCu3(PO4)4 (mp-760136) | 0.6107 | 0.090 | 5 |
Li5Co2Cu2(PO4)4 (mp-766608) | 0.4899 | 0.061 | 5 |
Li7CuAs4ClO14 (mp-769204) | 0.5472 | 0.074 | 5 |
Li3Mn2P2(O4F)2 (mp-763234) | 0.6137 | 0.024 | 5 |
Li12CoNi3P4(CO7)4 (mp-767857) | 0.7403 | 0.036 | 6 |
Explore more synthesis descriptions for materials of composition LiMnPO4.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-7.1374 eV |
Corrected Energy-1306.8423 eV
-1306.8423 eV = -1199.0820 eV (uncorrected energy) - 67.4198 eV (MP Anion Correction) - 40.3404 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)