Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.670 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.182 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2FeSiO4 + Fe2SiO4 + SiO2 |
Band Gap4.093 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 -1> | 297.8 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 126.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 205.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 205.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 257.2 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 217.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 289.6 |
InAs (mp-20305) | <1 0 0> | <1 -1 -1> | 268.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 182.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 326.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 257.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 257.2 |
Te2W (mp-22693) | <0 1 1> | <1 -1 0> | 299.2 |
Te2Mo (mp-602) | <1 0 0> | <0 1 -1> | 210.5 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 277.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 308.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 303.3 |
AlN (mp-661) | <1 0 0> | <1 1 -1> | 297.8 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 217.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 257.2 |
GaAs (mp-2534) | <1 1 1> | <0 1 -1> | 280.6 |
BN (mp-984) | <0 0 1> | <1 -1 0> | 299.2 |
BN (mp-984) | <1 1 0> | <1 -1 -1> | 268.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 277.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 154.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 175.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 217.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 326.1 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 277.5 |
InAs (mp-20305) | <1 1 0> | <0 1 -1> | 210.5 |
MoS2 (mp-1434) | <1 0 0> | <1 -1 -1> | 268.1 |
ZnSe (mp-1190) | <1 1 1> | <0 1 -1> | 280.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 205.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 144.8 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 303.3 |
Al (mp-134) | <1 1 1> | <1 0 -1> | 144.8 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 -1> | 217.2 |
LiGaO2 (mp-5854) | <1 0 0> | <1 -1 -1> | 178.8 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 -1> | 289.6 |
LiF (mp-1138) | <1 0 0> | <1 -1 0> | 149.6 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 144.8 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 257.2 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 242.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 -1> | 280.6 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 242.7 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 182.0 |
GaSe (mp-1943) | <1 0 0> | <1 1 0> | 202.7 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 289.6 |
BN (mp-984) | <1 0 1> | <1 0 0> | 260.9 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 303.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnSiO3 (mp-565815) | 0.4769 | 0.007 | 3 |
MnSiO3 (mp-19528) | 0.4718 | 0.007 | 3 |
MgSiO3 (mp-1020125) | 0.4666 | 0.029 | 3 |
MgSiO3 (mp-1020361) | 0.4790 | 0.028 | 3 |
MgSiO3 (mp-1020117) | 0.4746 | 0.029 | 3 |
Li2Mn2Si4O11 (mp-767711) | 0.1192 | 0.104 | 4 |
Li2Fe4Si4O13 (mp-761705) | 0.4360 | 0.269 | 4 |
Li2Mn4Si4O13 (mp-861609) | 0.4355 | 0.011 | 4 |
Li2Mg2Si4O11 (mp-561336) | 0.0929 | 0.015 | 4 |
Li2V2Si4O11 (mp-761443) | 0.2454 | 0.013 | 4 |
Li6MnV3(PO4)6 (mp-778914) | 0.5784 | 0.228 | 5 |
Na6Al4Fe(Si4O13)2 (mp-39647) | 0.5963 | 0.043 | 5 |
Li3MnV(PO4)3 (mp-780675) | 0.5773 | 0.222 | 5 |
Li6MnV3(PO4)6 (mp-779387) | 0.5938 | 0.232 | 5 |
Na6Al4Fe(Si4O13)2 (mp-698697) | 0.5781 | 0.043 | 5 |
Li4Mn3CuNi2(PO4)6 (mp-775323) | 0.6953 | 0.080 | 6 |
CaMg2TiAl2SiO10 (mp-534863) | 0.6783 | 0.026 | 6 |
Li4Mn2VNi3(PO4)6 (mp-770417) | 0.7017 | 0.075 | 6 |
Li4TiCo2Ni3(PO4)6 (mp-778251) | 0.7027 | 0.203 | 6 |
Li4TiCu2Ni3(PO4)6 (mp-776613) | 0.7039 | 0.101 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6294 | 0.068 | 7 |
KNa2LiTi2Fe2(SiO3)8 (mp-542926) | 0.7372 | 0.071 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Si O |
Final Energy/Atom-7.0749 eV |
Corrected Energy-292.9828 eV
Uncorrected energy = -268.8448 eV
Composition-based energy adjustment (-0.687 eV/atom x 22.0 atoms) = -15.1140 eV
Composition-based energy adjustment (-2.256 eV/atom x 4.0 atoms) = -9.0240 eV
Corrected energy = -292.9828 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)