Final Magnetic Moment6.894 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.031 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.086 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu3(PO4)2 + Li2CuP2O7 + CuO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 268.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 195.8 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 201.0 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 201.0 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 174.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 261.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 87.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 261.7 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 87.2 |
BN (mp-984) | <0 0 1> | <0 1 0> | 268.1 |
BN (mp-984) | <1 1 0> | <1 0 0> | 261.7 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 261.7 |
MoS2 (mp-1434) | <1 0 1> | <1 0 0> | 261.7 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 220.0 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 154.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 1> | 195.8 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 154.5 |
C (mp-66) | <1 1 0> | <0 1 0> | 201.0 |
C (mp-66) | <1 0 0> | <0 1 0> | 268.1 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 134.0 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 134.0 |
PbSe (mp-2201) | <1 0 0> | <1 0 1> | 195.8 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 0> | 220.0 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 261.7 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 261.7 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 268.1 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 87.2 |
WS2 (mp-224) | <1 1 0> | <0 0 1> | 154.5 |
CdSe (mp-2691) | <1 0 0> | <1 0 1> | 195.8 |
C (mp-48) | <0 0 1> | <0 1 1> | 168.4 |
C (mp-48) | <1 1 0> | <1 0 0> | 261.7 |
YAlO3 (mp-3792) | <1 1 1> | <1 0 0> | 261.7 |
SiC (mp-8062) | <1 1 1> | <1 0 0> | 261.7 |
MgF2 (mp-1249) | <1 0 1> | <1 0 -1> | 157.0 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 268.1 |
ZnO (mp-2133) | <1 0 0> | <0 1 0> | 268.1 |
ZnO (mp-2133) | <1 0 1> | <0 1 0> | 201.0 |
ZnO (mp-2133) | <1 1 1> | <1 1 0> | 220.0 |
TiO2 (mp-390) | <1 0 1> | <0 1 0> | 201.0 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 87.2 |
GaSb (mp-1156) | <1 0 0> | <1 0 1> | 195.8 |
Cu (mp-30) | <1 1 0> | <0 1 0> | 201.0 |
LiAlO2 (mp-3427) | <1 0 0> | <1 0 0> | 261.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr4P2O9 (mp-773396) | 0.5084 | 0.230 | 3 |
NaPO3 (mp-558192) | 0.5866 | 0.006 | 3 |
Ca5Ge3O11 (mp-774105) | 0.5750 | 0.016 | 3 |
Na2Mo2O7 (mp-25774) | 0.5923 | 0.000 | 3 |
Mn4(PO4)3 (mp-32010) | 0.5919 | 0.142 | 3 |
LiCu4(PO4)3 (mp-762116) | 0.4851 | 0.070 | 4 |
Li4Si4Bi2O13 (mp-756672) | 0.4600 | 0.077 | 4 |
V2Zn(PO4)2 (mvc-10167) | 0.4834 | 0.075 | 4 |
CaV2(PO4)2 (mvc-9882) | 0.4354 | 0.093 | 4 |
Li3Sb3(PO4)4 (mp-759918) | 0.4235 | 0.053 | 4 |
LiMn3P2(HO3)4 (mp-763726) | 0.4613 | 0.479 | 5 |
Na2LiVPO6 (mp-763825) | 0.5545 | 0.094 | 5 |
SrMgCo(PO4)2 (mvc-2989) | 0.5537 | 0.014 | 5 |
SrMgNi(PO4)2 (mvc-2996) | 0.5157 | 0.019 | 5 |
SrMgFe(PO4)2 (mvc-3019) | 0.5505 | 0.015 | 5 |
Li4Mn3NbV2(PO4)6 (mp-770640) | 0.6155 | 0.095 | 6 |
LiMnVP2(HO5)2 (mp-766999) | 0.6345 | 0.039 | 6 |
Li4Cr2Ni3Sn(PO4)6 (mp-778614) | 0.6344 | 0.183 | 6 |
Li4Mn3NbCr2(PO4)6 (mp-776566) | 0.5848 | 0.102 | 6 |
Li4Mn2Fe3Sb(PO4)6 (mp-776752) | 0.6136 | 3.420 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv P O |
Final Energy/Atom-6.1945 eV |
Corrected Energy-270.8290 eV
-270.8290 eV = -253.9740 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)