Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.820 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.736 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4332 [212] |
HallP 4acd 2ab 3 |
Point Group432 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 204.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 272.8 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 289.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 68.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 96.5 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 272.8 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 289.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 96.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 68.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 272.8 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 272.8 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 289.4 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 192.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 68.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 272.8 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 96.5 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 118.1 |
Al (mp-134) | <1 0 0> | <1 0 0> | 272.8 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 204.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 136.4 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 192.9 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 289.4 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 204.6 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 289.4 |
C (mp-66) | <1 1 0> | <1 1 0> | 289.4 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 96.5 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 204.6 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 272.8 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 136.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 1 0> | 192.9 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 272.8 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 68.2 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 96.5 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 192.9 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 192.9 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 272.8 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 272.8 |
Ga2O3 (mp-886) | <0 1 0> | <1 1 0> | 289.4 |
Ga2O3 (mp-886) | <1 0 0> | <1 1 0> | 289.4 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 289.4 |
Si (mp-149) | <1 0 0> | <1 0 0> | 272.8 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 136.4 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 272.8 |
Au (mp-81) | <1 0 0> | <1 0 0> | 68.2 |
Au (mp-81) | <1 1 0> | <1 1 0> | 96.5 |
Au (mp-81) | <1 1 1> | <1 1 1> | 118.1 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 1 0> | 96.5 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 272.8 |
Ge (mp-32) | <1 1 0> | <1 1 0> | 96.5 |
MgAl2O4 (mp-3536) | <1 0 0> | <1 0 0> | 68.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn3Cu3O8 (mp-652534) | 0.1004 | 0.021 | 3 |
Fe9Cu3O16 (mp-868046) | 0.1206 | 0.141 | 3 |
LiCr2O4 (mp-774032) | 0.1183 | 0.023 | 3 |
Fe2CoO4 (mp-765860) | 0.1085 | 0.055 | 3 |
Co2CuO4 (mp-39091) | 0.1118 | 0.020 | 3 |
Li2MnFe3O8 (mp-775732) | 0.1105 | 0.025 | 4 |
Li2Ni3SbO8 (mp-775726) | 0.1129 | 0.015 | 4 |
Li2MnCr3O8 (mp-774951) | 0.1073 | 0.005 | 4 |
Li2NbV3O8 (mp-774010) | 0.1102 | 0.006 | 4 |
Li2Ti3NbO8 (mp-776215) | 0.1037 | 0.053 | 4 |
Hf3N4 (mp-755988) | 0.2429 | 0.016 | 2 |
In3S4 (mp-556597) | 0.2198 | 0.042 | 2 |
Ni3S4 (mp-1050) | 0.2089 | 0.000 | 2 |
Sn3N4 (mp-16031) | 0.2248 | 0.000 | 2 |
Ge3N4 (mp-476) | 0.2365 | 0.109 | 2 |
Li4Cr2Fe3Co3O16 (mp-775698) | 0.2734 | 0.894 | 5 |
Li4Mn2Fe3Co3O16 (mp-761441) | 0.2697 | 0.079 | 5 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.2161 | 0.019 | 5 |
Li4Mn3Cr3(CuO8)2 (mp-765456) | 0.2624 | 0.080 | 5 |
Li4Cr3Cu3(SbO8)2 (mp-783908) | 0.2620 | 0.040 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7299 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.7319 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.7374 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.7306 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7353 | 0.661 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co Sb O |
Final Energy/Atom-5.9353 eV |
Corrected Energy-377.3386 eV
-377.3386 eV = -332.3773 eV (uncorrected energy) - 22.4880 eV (MP Advanced Correction) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)