Final Magnetic Moment1.994 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.593 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.071 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiV2(PO4)3 |
Band Gap1.220 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 109.8 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 291.0 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 339.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 194.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 339.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 97.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 145.5 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 263.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 339.4 |
SiO2 (mp-6930) | <1 0 1> | <1 1 -1> | 177.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 263.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 194.0 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 106.9 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 339.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 145.5 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 213.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 109.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 219.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 242.5 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 242.5 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 242.5 |
BN (mp-984) | <1 0 1> | <0 1 0> | 141.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 291.0 |
BN (mp-984) | <1 1 1> | <1 0 0> | 242.5 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 339.4 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 339.4 |
TeO2 (mp-2125) | <1 0 0> | <1 0 -1> | 213.9 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 97.0 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 -1> | 213.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 109.8 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 242.5 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 109.8 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 339.4 |
C (mp-66) | <1 0 0> | <0 1 0> | 141.0 |
C (mp-66) | <1 1 0> | <1 0 -1> | 106.9 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 145.5 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 194.0 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 97.0 |
InP (mp-20351) | <1 0 0> | <1 0 -1> | 106.9 |
PbS (mp-21276) | <1 0 0> | <1 0 -1> | 106.9 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 339.4 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 194.0 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 263.7 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 242.5 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 194.0 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 242.5 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 0> | 145.5 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 109.8 |
Au (mp-81) | <1 0 0> | <1 0 0> | 242.5 |
Au (mp-81) | <1 1 1> | <1 0 0> | 242.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-771363) | 0.4744 | 0.025 | 3 |
Sb2(SeO4)3 (mp-779462) | 0.4518 | 0.087 | 3 |
Mn2(SO4)3 (mp-771368) | 0.4673 | 0.000 | 3 |
Cu2(SO4)3 (mp-768512) | 0.4686 | 0.038 | 3 |
MoPO5 (mvc-9141) | 0.4682 | 0.070 | 3 |
V4Zn(PO4)6 (mvc-12911) | 0.4002 | 0.038 | 4 |
VHg4P2O9 (mp-565729) | 0.3967 | 0.000 | 4 |
AgMoPO6 (mp-19569) | 0.4332 | 0.000 | 4 |
LiCr2(PO4)3 (mp-778036) | 0.2703 | 0.171 | 4 |
LiV2(PO4)3 (mp-32478) | 0.3562 | 0.088 | 4 |
Mo4O11 (mp-565865) | 0.6851 | 0.026 | 2 |
V5O12 (mp-778252) | 0.7465 | 0.024 | 2 |
K2CoP2WO10 (mp-645301) | 0.4669 | 0.062 | 5 |
MnCr3Te2(PO4)6 (mp-765202) | 0.4597 | 0.089 | 5 |
MgTiAg(PO4)3 (mvc-8846) | 0.4618 | 0.088 | 5 |
CaTiAg(PO4)3 (mvc-8845) | 0.4459 | 0.061 | 5 |
TiZnAg(PO4)3 (mvc-8854) | 0.4556 | 0.096 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.5886 | 0.080 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.5731 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.5992 | 0.015 | 6 |
Na2Li4Ti3Al(PO4)6 (mp-769069) | 0.6203 | 0.087 | 6 |
Li4TiMn3Cr2(PO4)6 (mp-778261) | 0.6286 | 0.081 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.2545 eV |
Corrected Energy-284.7448 eV
-284.7448 eV = -261.1618 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)