Final Magnetic Moment0.057 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.225 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.070 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2CuP2O7 + Cu2O + SbPO4 + CuO + Li3PO4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm [6] |
HallP 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 181.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 196.5 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 217.5 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 72.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 272.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 272.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 324.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 121.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 333.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 212.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 181.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 151.5 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 344.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 272.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 288.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 324.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 121.2 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 290.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 288.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 217.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 212.1 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 194.8 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 217.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 333.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 242.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 259.8 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 217.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 259.8 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 288.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 242.4 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 259.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 64.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 324.7 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 194.8 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 194.8 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 90.9 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 272.7 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 64.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 333.3 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 194.8 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 194.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 259.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 333.3 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 196.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 242.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 272.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 212.1 |
BN (mp-984) | <1 1 0> | <0 0 1> | 272.7 |
BN (mp-984) | <1 1 1> | <0 1 0> | 245.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 121.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn4SiO7 (mp-19591) | 0.4860 | 0.043 | 3 |
Mn2SiO4 (mp-18928) | 0.4756 | 0.000 | 3 |
Fe2SiO4 (mp-510587) | 0.4622 | 0.000 | 3 |
Ca2GeO4 (mp-560647) | 0.4928 | 0.000 | 3 |
Ca2SiO4 (mp-4481) | 0.4591 | 0.000 | 3 |
Li3Mn(PO4)2 (mp-771633) | 0.3204 | 0.020 | 4 |
Li5Mn3(PO4)4 (mp-771623) | 0.3279 | 0.012 | 4 |
Li3Sb(PO4)2 (mp-774714) | 0.3277 | 0.061 | 4 |
Li7Mn(PO4)4 (mp-850224) | 0.2880 | 0.068 | 4 |
LiCdPO4 (mp-556786) | 0.2989 | 0.000 | 4 |
Li4Cu3Bi(PO4)4 (mp-765628) | 0.2224 | 0.070 | 5 |
Li4Mn3Sn(PO4)4 (mp-767327) | 0.3117 | 0.033 | 5 |
Li4MnCu3(PO4)4 (mp-767040) | 0.2497 | 0.027 | 5 |
Li2NiSn(PO4)2 (mp-773195) | 0.2914 | 0.149 | 5 |
Li4Cu3Ni(PO4)4 (mp-761659) | 0.3027 | 0.029 | 5 |
Li3MnFeCo(PO4)3 (mp-764804) | 0.4063 | 0.043 | 6 |
Li3MnFeCo(PO4)3 (mp-764912) | 0.3936 | 0.282 | 6 |
Li3MnFeCo(PO4)3 (mp-764708) | 0.3902 | 0.599 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.4039 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.3977 | 0.466 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv Sb P O |
Final Energy/Atom-6.2838 eV |
Corrected Energy-187.1828 eV
-187.1828 eV = -175.9462 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|