Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.196 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.124 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNiPO4 |
Band Gap3.461 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP65 [170] |
HallP 65 |
Point Group6 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 254.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 84.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 169.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 254.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 84.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 84.9 |
C (mp-66) | <1 0 0> | <0 0 1> | 254.7 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 169.8 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 254.7 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 84.9 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 254.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 254.7 |
C (mp-66) | <1 1 0> | <0 0 1> | 254.7 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 254.7 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 169.8 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 254.7 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 84.9 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 254.7 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 169.8 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 254.7 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 254.7 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 254.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbV4O8 (mp-690170) | 0.6237 | 0.260 | 3 |
Mg3(AsO4)2 (mp-770734) | 0.4702 | 0.065 | 3 |
MgSiO3 (mp-642210) | 0.5932 | 0.165 | 3 |
Fe3(PO4)2 (mp-636647) | 0.6189 | 0.000 | 3 |
Ni3(PO4)2 (mp-771911) | 0.5602 | 0.192 | 3 |
LiCuPO4 (mp-758918) | 0.1993 | 0.090 | 4 |
Li2CoP2O7 (mp-778917) | 0.4062 | 0.155 | 4 |
LiFeSiO4 (mp-762686) | 0.3674 | 0.088 | 4 |
LiNiPO4 (mp-772673) | 0.3816 | 0.058 | 4 |
LiCoPO4 (mp-761821) | 0.3862 | 0.042 | 4 |
Li3CoPCO7 (mp-775230) | 0.6963 | 0.068 | 5 |
Li3NiPCO7 (mp-767326) | 0.6780 | 0.073 | 5 |
NaLiZnP2O7 (mp-676483) | 0.5508 | 0.002 | 5 |
Li3NiPCO7 (mp-767870) | 0.6933 | 0.139 | 5 |
Li3NiPCO7 (mp-767867) | 0.6976 | 0.119 | 5 |
KMg3AlSi3(O5F)2 (mp-684841) | 0.6944 | 0.230 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv P O |
Final Energy/Atom-6.1852 eV |
Corrected Energy-1158.4636 eV
-1158.4636 eV = -1039.1078 eV (uncorrected energy) - 67.4198 eV (MP Anion Correction) - 51.9360 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)