Final Magnetic Moment14.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.434 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.078 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVO2 + V2O3 |
Band Gap1.082 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 269.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 202.4 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 253.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 235.9 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 276.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 141.5 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 303.6 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 279.2 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 253.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 253.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 330.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 235.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 141.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 141.5 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 276.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 188.7 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 151.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 269.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 218.5 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 276.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 253.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 283.1 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 151.8 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 330.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 330.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 202.4 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 202.4 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 283.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 330.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 94.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 330.2 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 179.7 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 283.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 47.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 283.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 141.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 330.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 141.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 330.2 |
Al (mp-134) | <1 1 0> | <0 1 0> | 202.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 253.0 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 202.4 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 202.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 330.2 |
Al (mp-134) | <1 1 1> | <0 1 0> | 253.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 141.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 235.9 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 283.1 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 47.2 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 141.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Fe7O12 (mp-762465) | 0.1841 | 0.107 | 3 |
Li5Fe5O12 (mp-762602) | 0.1832 | 0.694 | 3 |
Li8V11O22 (mp-768084) | 0.2184 | 0.043 | 3 |
Li5V5O12 (mp-762939) | 0.1807 | 0.156 | 3 |
Li3Fe2Ni5O12 (mp-997540) | 0.1330 | 0.077 | 4 |
Li2Cr2FeO6 (mp-782636) | 0.1504 | 0.804 | 4 |
Li2Mn(FeO3)2 (mp-762835) | 0.1446 | 0.071 | 4 |
Li2V2CrO6 (mp-849330) | 0.1400 | 0.482 | 4 |
Li2Fe2CuO6 (mp-849448) | 0.1311 | 0.075 | 4 |
Ni6O7 (mp-767815) | 0.2286 | 0.047 | 2 |
Ni5O6 (mp-782702) | 0.2623 | 0.041 | 2 |
V6C5 (mp-28731) | 0.2526 | 0.000 | 2 |
Fe7O8 (mp-715333) | 0.3126 | 0.064 | 2 |
Ni6Cl7 (mp-1022720) | 0.2673 | 0.167 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.4127 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O |
Final Energy/Atom-7.3643 eV |
Corrected Energy-182.2171 eV
-182.2171 eV = -162.0156 eV (uncorrected energy) - 11.7740 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)