Final Magnetic Moment1.991 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.567 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.024 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToP3(WO6)2 + Li3PO4 + W |
Band Gap3.256 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3 [147] |
Hall-P 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 187.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 270.9 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 189.8 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 303.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 375.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 75.9 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 173.2 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 263.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 208.4 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 263.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 265.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 104.2 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 137.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 270.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 270.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 189.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 166.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 189.8 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 259.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 62.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 151.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 20.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 83.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 216.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 375.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 275.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 187.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 62.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 62.5 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 227.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 333.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 83.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 229.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 333.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 341.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 83.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 265.7 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 263.0 |
Te2W (mp-22693) | <0 1 1> | <1 1 1> | 275.9 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 303.1 |
TePb (mp-19717) | <1 1 1> | <1 0 1> | 303.1 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 187.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 104.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 145.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 270.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 145.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 270.9 |
BN (mp-984) | <1 0 0> | <1 0 0> | 38.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 229.3 |
BN (mp-984) | <1 1 0> | <1 1 0> | 65.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe4As2O11 (mp-31803) | 0.7459 | 0.136 | 3 |
MgCrO4 (mp-540704) | 0.7457 | 0.902 | 3 |
Li2Cr(PO4)2 (mp-764976) | 0.1888 | 0.109 | 4 |
Li2Nb(PO4)2 (mp-760377) | 0.1074 | 0.102 | 4 |
Li2V(PO4)2 (mp-763559) | 0.1435 | 0.065 | 4 |
Li2Fe(PO4)2 (mp-762553) | 0.4218 | 0.252 | 4 |
Li2Mo(PO4)2 (mp-585209) | 0.3294 | 0.023 | 4 |
Al9Fe2Si4HO24 (mp-744386) | 0.6672 | 0.142 | 5 |
LiMn2P2HO8 (mp-779995) | 0.6246 | 0.036 | 5 |
Li3MnP2HO8 (mp-763836) | 0.6520 | 0.212 | 5 |
Li6MnV3(PO4)6 (mp-778701) | 0.6678 | 0.117 | 5 |
LiFe2P2HO8 (mp-773622) | 0.6209 | 0.032 | 5 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.7470 | 0.015 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv P W_pv O |
Final Energy/Atom-6.9678 eV |
Corrected Energy-100.5509 eV
-100.5509 eV = -90.5816 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 4.3510 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)