Final Magnetic Moment3.424 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.716 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.123 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi(CoO2)2 + Li2CO3 + CO2 + CoCO3 |
Band Gap0.819 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCcc2 [37] |
HallC 2 2c |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 1 0> | 190.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 168.2 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 47.6 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 119.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 238.2 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 333.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 95.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 128.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 168.2 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 47.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 47.6 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 333.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 119.4 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 238.2 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 285.9 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 257.1 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 238.2 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 47.6 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 238.2 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 333.5 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 153.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 142.9 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 190.6 |
BN (mp-984) | <0 0 1> | <0 1 0> | 190.6 |
BN (mp-984) | <1 0 1> | <0 1 0> | 238.2 |
BN (mp-984) | <1 1 0> | <0 1 0> | 333.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 47.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 168.2 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 238.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 96.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 333.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 238.2 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 238.2 |
Al (mp-134) | <1 1 1> | <1 1 0> | 290.0 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 128.5 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 238.2 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 47.6 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 190.6 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 238.8 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 95.3 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 238.2 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 190.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 333.5 |
SiC (mp-7631) | <1 1 0> | <0 1 1> | 257.1 |
SiC (mp-7631) | <1 1 1> | <0 1 1> | 257.1 |
BN (mp-984) | <1 1 1> | <0 1 0> | 238.2 |
MgO (mp-1265) | <1 0 0> | <1 1 0> | 290.0 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 333.5 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 238.2 |
Al (mp-134) | <1 0 0> | <1 1 0> | 96.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2Ti2O5 (mp-779477) | 0.6952 | 0.026 | 3 |
Zn3(BO3)2 (mp-542833) | 0.6540 | 0.019 | 3 |
CuCO3 (mp-760536) | 0.6535 | 0.132 | 3 |
Zn3(BO3)2 (mp-557683) | 0.6915 | 0.013 | 3 |
Zn3(BO3)2 (mp-559949) | 0.6610 | 0.019 | 3 |
LiFeCO4 (mp-762000) | 0.2241 | 0.386 | 4 |
LiCu2(CO3)2 (mp-760546) | 0.5401 | 0.065 | 4 |
CaGaBO4 (mp-557855) | 0.5438 | 0.000 | 4 |
CaAlBO4 (mp-559759) | 0.4168 | 0.000 | 4 |
BaZn2(BO3)2 (mp-557974) | 0.5430 | 0.013 | 4 |
Li3BePCO7 (mp-771341) | 0.5372 | 0.051 | 5 |
Li3TlPCO7 (mp-771334) | 0.4910 | 0.110 | 5 |
Li3CrPCO7 (mp-767343) | 0.5943 | 0.084 | 5 |
Li3CrPCO7 (mp-767898) | 0.5917 | 0.203 | 5 |
Li3CrPCO7 (mp-767892) | 0.5918 | 0.211 | 5 |
ZnPH7C2N4O5 (mp-699466) | 0.7306 | 0.017 | 6 |
Na3LiMnBPO7 (mp-763842) | 0.7090 | 0.077 | 6 |
NaLiMnPCO7 (mp-763833) | 0.7035 | 0.000 | 6 |
NaPH3C2N3O4 (mp-765959) | 0.6975 | 0.031 | 6 |
ZnP2H14C2(NO)6 (mp-757310) | 0.6749 | 0.050 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co C O |
Final Energy/Atom-6.4807 eV |
Corrected Energy-200.1924 eV
-200.1924 eV = -181.4598 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 7.4960 eV (MP Advanced Correction)
|